Supported glove having an abrasion resistant nitrile coating
US-2016262469-A1 · Sep 15, 2016 · US
US11325356B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11325356-B2 |
| Application number | US-201716337104-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 19, 2017 |
| Priority date | Sep 30, 2016 |
| Publication date | May 10, 2022 |
| Grant date | May 10, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of producing a laminated body, the method including a coagulant solution deposition step of depositing a coagulant solution on a fiber substrate, and a coagulation step of forming a polymer layer on the fiber substrate by bringing a polymer latex into contact with the fiber substrate having the coagulant solution deposited thereon to cause a polymer to coagulate. As the coagulant solution, a solution obtained by dissolving or dispersing 0.2 to 7.0% by weight of a metal salt as a coagulant and 0.1 to 7.0% by weight of an organic acid in a solvent is used. In the method of producing a laminated body, the metal salt is a polyvalent metal salt. In the method of producing a laminated body, the organic acid is an organic acid having at least one group selected from a carboxyl group, a sulfo group, a hydroxy group, and a thiol group.
Opening claim text (preview).
The invention claimed is: 1. A method of producing a laminated body, the method comprising: a coagulant solution deposition step of depositing a coagulant solution on a fiber substrate; and a coagulation step of forming a polymer layer on the fiber substrate by bringing a polymer latex into contact with the fiber substrate having the coagulant solution deposited thereon to cause a polymer to coagulate, wherein as the coagulant solution, a solution obtained by dissolving or dispersing 0.2 to 1.0% by weight of a metal salt as a coagulant and 0.1 to 3.0% by weight of an organic acid in a solvent is used, and the metal salt is calcium nitrate and the organic acid is acetic acid. 2. The method of producing a laminated body according to claim 1 , wherein a polymer constituting the polymer latex is a nitrile rubber. 3. The method of producing a laminated body according to claim 1 , wherein in the coagulation step, the polymer layer is formed so that a permeated polymer layer, which, of the polymer layer, is a portion having permeated into the fiber substrate, has a thickness of 0.05 to 0.6 mm. 4. The method of producing a laminated body according to claim 1 , wherein in the coagulation step, the polymer layer is formed so that a top surface polymer layer, which, of the polymer layer, is a portion having not permeated into the fiber substrate, has a thickness of 0.05 to 0.6 mm. 5. A method of producing a protective glove using a laminated body obtained by the method of producing a laminated body according to claim 1 .
next to a fibrous or filamentary layer · CPC title
Halides of elements of Groups 4 or 14 of the Periodic Table, e.g. zirconyl chloride · CPC title
the macromolecular compounds being water soluble or water swellable, e.g. aqueous gels · CPC title
Fibrous or filamentary layer · CPC title
Acids; Salts thereof {(C08K3/16 takes precedence)} · CPC title
Related publications grouped by family.