Surfactant composition
US-2015126417-A1 · May 7, 2015 · US
US11293106B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11293106-B2 |
| Application number | US-201916722170-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 20, 2019 |
| Priority date | Dec 20, 2018 |
| Publication date | Apr 5, 2022 |
| Grant date | Apr 5, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Method of minimizing pitting corrosion at temperatures above 130° C., wherein said method comprises: providing an acidic fluid comprising an alkylsulfonic acid; providing at least one corrosion inhibitor compound comprising an organic compound comprising at least two aldehyde functional groups; combining said acidic fluid with said at least one corrosion inhibitor compound; exposing said mixed fluid to a metallic surface at a temperature of at least 130° C.; and allowing said mixed fluid sufficient time of exposure to a metal to accomplish a pre-determined function.
Opening claim text (preview).
The invention claimed is: 1. An alkylsulfonic acid composition comprising an alkylsulfonic acid and a corrosion inhibitor composition, said corrosion inhibitor composition comprising: an organic compound comprising at least two aldehyde functional groups; optionally, a propargyl alcohol; an anionic surfactant which is a dicarboxylic surfactant; at least one amphoteric surfactant; and a solvent; wherein the alkylsulfonic acid is present in an amount ranging from 1 wt % to 50 wt % of the sulfonic acid composition in water. 2. The alkylsulfonic acid composition as claimed in claim 1 , wherein the alkylsulfonic acid is methanesulfonic acid. 3. The alkylsulfonic acid composition as claimed in claim 1 , wherein the at least one amphoteric surfactant is selected from the group consisting of: a sultaine surfactant; a betaine surfactant; and combinations thereof. 4. The alkylsulfonic acid composition as claimed in claim 1 , wherein at least one amphoteric surfactant is a sultaine surfactant and betaine surfactant and are selected from the group consisting of: an amido betaine surfactant; an amido sultaine surfactant; and combinations thereof. 5. The alkylsulfonic acid composition as claimed in claim 1 , wherein the at least one amphoteric surfactant is an amido betaine surfactant and is selected from the group consisting of: an amido betaine comprising a hydrophobic tail from C8 to C16. 6. The alkylsulfonic acid composition as claimed in claim 1 , wherein the at least one amphoteric surfactant is cocamidobetaine. 7. The alkylsulfonic acid composition as claimed in claim 1 , further comprising an anionic surfactant which is a carboxylic surfactant. 8. The alkylsulfonic acid composition as claimed in claim 1 , wherein said anionic surfactant is a dicarboxylic surfactant comprising a hydrophobic tail ranging from C8 to C16. 9. The alkylsulfonic acid composition as claimed in claim 1 , wherein said anionic surfactant is an iminodicarboxylate including sodium lauriminodipropionate. 10. The alkylsulfonic acid composition as claimed in claim 1 , wherein the surfactant is selected from the group consisting of: cocamidopropyl betaine; β-Alanine, N-(2-carboxyethyl)-N-dodecyl-, sodium salt (1:1); and a combination thereof. 11. The alkylsulfonic acid composition as claimed in claim 1 , wherein the propargyl alcohol is present in an amount ranging from 20% to 55% by volume of the total weight of the corrosion inhibitor composition. 12. The alkylsulfonic acid composition as claimed in claim 1 , wherein the surfactant is present in an amount ranging from 2% to 20% by volume of the total weight of the corrosion inhibitor composition. 13. The alkylsulfonic acid composition as claimed in claim 1 , wherein the solvent is present in an amount ranging from 10% to 45% by volume of the total weight of the corrosion inhibitor composition.
containing organic compounds · CPC title
containing surfactants · CPC title
in markedly acid liquids · CPC title
combined with additives added for specific purposes · CPC title
Anticorrosion additives · CPC title