Methods of manufacturing polyolefin drag reducing agents
US-2019382511-A1 · Dec 19, 2019 · US
US11248748B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11248748-B2 |
| Application number | US-202016892834-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jun 4, 2020 |
| Priority date | Jun 14, 2019 |
| Publication date | Feb 15, 2022 |
| Grant date | Feb 15, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A drag reducing composition comprises a sealed temporary container; and a drag reducing agent and up to 20 weight percent of a dispersing fluid disposed in the sealed temporary container. The drag reducing agent comprises polyolefin particles having a particle size of about 10 to about 2,000 microns; and the dispersing fluid comprising water, an alcohol, a hydrocarbon, or a combination comprising at least one of the foregoing.
Opening claim text (preview).
What is claimed is: 1. A drag reducing composition comprising: a sealed temporary container; and a drag reducing agent and up to 20 weight percent of a dispersing fluid disposed in the sealed temporary container; wherein the drag reducing agent comprises polyolefin particles having a particle size of about 10 to about 2,000 microns; the dispersing fluid comprises water, an alcohol, a hydrocarbon, or a combination comprising at least one of the foregoing; the temporary container comprises a container material, which includes a polyethylene, a polypropylene, an ethylene propylene copolymer, a polystyrene, a polylactic acid, a polyamide, a polyester, a polystyrene, an ethylene vinyl acetate copolymer, an ethylene vinyl alcohol copolymer, a polyvinylpyrrolidone, an ethylene vinylpyrrolidone copolymer, a vinylpyrrolidone vinyl acetate copolymer, a polyvinyl acetate, a polyvinyl alcohol, a polyethylene oxide, a polyethylene glycol, polyvinylidene chloride, a polysaccharide or its derivative, or a combination comprising at least one of the foregoing; and the weight percent is based on the total weight of the drag reducing composition, and wherein the temporary container has a thickness of about 1 to about 1,000 microns. 2. The drag reducing composition of claim 1 , wherein the drag reducing agent comprises a plurality of first polyolefin particles; and a plurality of second polyolefin particles different from the first polyolefin particles. 3. The drag reducing composition of claim 2 , wherein the first polyolefin particles have a particle size of about 10 to about 200 microns and the second polyolefin particles have a particle size of about 200 to about 2,000 microns. 4. The drag reducing composition of claim 2 , wherein the first polyolefin particles have a weight average molecular weight of about 50,000 to about 20,000,000 and the second polyolefin particles have a weight average molecular weight of about 1,000,000 to more than 30,000,000. 5. The drag reducing composition of claim 1 , further comprising an anti-agglomeration agent disposed in the sealed temporary container, wherein the anti-agglomeration agent comprises a salt of fatty acids having 12-20 carbon atoms, a polyethylene glycol or a polyethylene oxide with molecular weight 400 to 20,000,000 Daltons, a methoxylated polyethylene glycol, a polyacrylamide or a chemically modified polyacrylamide with molecular weight 400 to 30,000,000 Daltons, a linear primary alcohol having 12 to 60 carbon atoms, a polyethylene wax with molecular weight 400 to 3000 Daltons, a linear primary alcohol ethoxylate with molecular weight 500 to 5000 Daltons, ethylene-bis-stearamide, an inorganic clay, a silicone, or a combination comprising at least one of the foregoing. 6. A drag reducing composition comprising: a sealed temporary container; and a drag reducing agent and up to 20 weight percent of a dispersing fluid disposed in the sealed temporary container; wherein the drag reducing agent comprises polyolefin particles having a particle size of about 10 to about 2,000 microns; the dispersing fluid comprises water, an alcohol, a hydrocarbon, or a combination comprising at least one of the foregoing; the temporary container comprises a container material, which includes a polyethylene, a polypropylene, an ethylene propylene copolymer, a polystyrene, a polylactic acid, a polyamide, a polyester, a polystyrene, an ethylene vinyl acetate copolymer, an ethylene vinyl alcohol copolymer, a polyvinylpyrrolidone, an ethylene vinylpyrrolidone copolymer, a vinylpyrrolidone vinyl acetate copolymer, a polyvinyl acetate, a polyvinyl alcohol, a polyethylene oxide, a polyethylene glycol, polyvinylidene chloride, a polysaccharide or its derivative, or a combination comprising at least one of the foregoing; and the weight percent is based on the total weight of the drag reducing composition, and wherein the temporary container has two or more layers, and at least one layer comprises the container material. 7. The drag reducing composition of claim 6 , wherein each of the two or more layers independently comprises the container material. 8. A drag reducing composition comprising: a sealed temporary container; and a drag reducing agent and up to 20 weight percent of a dispersing fluid disposed in the sealed temporary container; wherein the drag reducing agent comprises polyolefin particles having a particle size of about 10 to about 2,000 microns; the dispersing fluid comprises water, an alcohol, a hydrocarbon, or a combination comprising at least one of the foregoing; the temporary container comprises a container material, which includes a polyethylene, a polypropylene, an ethylene propylene copolymer, a polystyrene, a polylactic acid, a polyamide, a polyester, a polystyrene, an ethylene vinyl acetate copolymer, an ethylene vinyl alcohol copolymer, a polyvinylpyrrolidone, an ethylene vinylpyrrolidone copolymer, a vinylpyrrolidone vinyl acetate copolymer, a polyvinyl acetate, a polyvinyl alcohol, a polyethylene oxide, a polyethylene glycol, polyvinylidene chloride, a polysaccharide or its derivative, or a combination comprising at least one of the foregoing; and the weight percent is based on the total weight of the drag reducing composition; and wherein the temporary container has an inner surface and an opposing outer surface, and a coating is disposed on at least one of the inner and outer surfaces of the temporary container, the coating comprising a wax, a silicone, or a combination comprising at least one of the foregoing. 9. The drag reducing composition of claim 8 , wherein the temporary container has a thickness of about 1 to about 1,000 microns. 10. A drag reducing composition comprising: a sealed temporary container; a drag reducing agent and up to 20 weight percent of a dispersing fluid disposed in the sealed temporary container; and a sealed pouch disposed inside the sealed temporary container; wherein the drag reducing agent comprises polyolefin particles having a particle size of about 10 to about 2,000 microns; the dispersing fluid comprises water, an alcohol, a hydrocarbon, or a combination comprising at least one of the foregoing; the temporary container comprises a container material, which includes a polyethylene, a polypropylene, an ethylene propylene copolymer, a polystyrene, a polylactic acid, a polyamide, a polyester, a polystyrene, an ethylene vinyl acetate copolymer, an ethylene vinyl alcohol copolymer, a polyvinylpyrrolidone, an ethylene vinylpyrrolidone copolymer, a vinylpyrrolidone vinyl acetate copolymer, a polyvinyl acetate, a polyvinyl alcohol, a polyethylene oxide, a polyethylene glycol, polyvinylidene chloride, a polysaccharide or its derivative, or a combination comprising at least one of the foregoing; and the weight percent is based on the total weight of the drag reducing composition. 11. The drag reducing composition of claim 1 , comprising a plurality of the sealed temporary container, wherein adjacent sealed temporary containers are connected, and the drag reducing agent is disposed in at least one of the plurality of the sealed temporary containers. 12. The drag reducing composition of claim 11 , wherein the plurality of the temporary containers form a chain having a length of greater than about 1 meter. 13. The drag reducing composition of claim 1 , wherein the polyolefin particles comprise a polyolefin homopolymer, a copolyolefin, a polyolefin copolymer, or a combination comprising at least one of the foregoing, and the polyolefin copolymer comprises first units derived from an olefin component and second units derived from styrene, a vinyl acetate, a vinylalkylene carboxylic e
Organic additives · CPC title
Oiliness; Film-strength; Anti-wear; Resistance to extreme pressure · CPC title
by mixing with another liquid {, i.e. diluting} · CPC title
Friction or drag reducing additives · CPC title
Lubricating compositions characterised by the additive being a macromolecular hydrocarbon or such hydrocarbon modified by oxidation · CPC title