Thermoplastic polyurethane elastomer, and preparation method, use and product thereof
US-2018291141-A1 · Oct 11, 2018 · US
US11242429B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11242429-B2 |
| Application number | US-202016736030-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jan 7, 2020 |
| Priority date | Jan 8, 2019 |
| Publication date | Feb 8, 2022 |
| Grant date | Feb 8, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A composition for an automotive interior skin, a method for manufacturing the same, and an automotive interior skin manufactured using the same. The composition for an automotive interior skin includes: 30 wt % to 70 wt % of a polyol compound; 5 wt % to 40 wt % of dicyclohexylmethane-4,4′-diisocyanate; and 5 wt % to 30 wt % of an aromatic glycol-based chain extender.
Opening claim text (preview).
What is claimed is: 1. A method for manufacturing a composition for an automotive interior skin, comprising the steps of: producing an intermediate molded body by kneading the composition for an automotive interior skin, comprising: 30 wt % to 70 wt % of a polyol component; 5 wt % to 40 wt % of dicyclohexylmethane-4,4′diisocyanate; and 5 wt % to 30 wt % of an aromatic glycol-based chain extender; producing a Pulverized Material by drying and Pulverizing the intermediate molded body at −60° C. or below; subjecting the Pulverized Material to first stirring at 80° C. or above; and subjecting the stirred Pulverized Material to second stirring. 2. The method of claim 1 , wherein the intermediate molded body is dried at a temperature of −60° C. to −190° C. 3. The method of claim 1 , wherein, after the step of producing the Pulverized Material, 0.05 parts by weight to 5 parts by weight of a drying agent is added to 100 parts by weight of the Pulverized Material, and the first stirring is performed. 4. The method of claim 1 , wherein the first stirring is performed by stirring the Pulverized Material at 500 rpm to 1,500 rpm and at 80° C. to 110° C., and the second stirring is performed by stirring the stirred Pulverized Material at 200 rpm to 1,000 rpm.
in dashboards · CPC title
Polycarbonates · CPC title
Making multilayered or multicoloured articles · CPC title
Polycondensates having carboxylic or carbonic ester groups in the main chain · CPC title
of foam · CPC title