Process for the preparation of sol-gel modified alternative Nafion-Silica composite membrane useful for polymer electrolyte fuel cell
US-8932782-B2 · Jan 13, 2015 · US
US11239485B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11239485-B2 |
| Application number | US-202016810282-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 5, 2020 |
| Priority date | Mar 27, 2015 |
| Publication date | Feb 1, 2022 |
| Grant date | Feb 1, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A process for the recovery of a perfluorosulphonic acid ionomer from a component comprising a perfluorosulphonic acid ionomer is disclosed, the process comprising immersing the component comprising the perfluorosulphonic acid ionomer in a solvent comprising an aliphatic diol and heating. Also disclosed is the use of the recovered perfluorosulphonic acid ionomer, for example in to prepared a proton conducting membrane or a catalyst ink.
Opening claim text (preview).
What is claimed: 1. A process for separating a membrane electrode assembly into components, said process comprising: (i) immersing the membrane electrode assembly in a solvent comprising a C1-8 aliphatic diol compound, wherein said diol compound comprises at least one —CH 2 OH group; and (ii) heating the membrane electrode assembly/solvent mix to a temperature of 90° C. to 150° C. to effect separation of the membrane electrode assembly components. 2. The process according to claim 1 , wherein the membrane electrode assembly is chopped or shredded prior to being immersed in the solvent. 3. The process according to claim 1 , said process comprising heating the membrane electrode assembly/solvent mix to a temperature of 90° C. to 120° C. 4. The process according to claim 1 , wherein the solvent further comprises a co-solvent. 5. A process for the recovery of one or more catalyst components from an original component selected from the group consisting of a perfluorosulphonic acid membrane, a catalyst coated membrane, an electrode and a membrane electrode assembly, said process comprising: (i) immersing the original component in a solvent comprising a C1-8 aliphatic diol compound, wherein said diol compound comprises at least one —CH 2 OH group; (ii) heating the component/solvent mix to a temperature of 90° C. to 150° C. to obtain a dispersion comprising solvent, one or more PFSA ionomers and the one or more catalyst components; and (iii) filtering the dispersion to separate the solvent and the one or more PFSA ionomers from the one of more catalyst components. 6. The process according to claim 5 , wherein the original component is chopped or shredded prior to being immersed in the solvent. 7. The process according to claim 5 , said process comprising heating the component/solvent mix to a temperature of 90° C. to 120° C. 8. The process according to claim 5 , wherein the solvent further comprises a co-solvent.