Aluminum alloy pipe-shaped hollow material and piping material for heat exchanger

US11220728B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-11220728-B2
Application numberUS-201816619536-A
CountryUS
Kind codeB2
Filing dateMay 28, 2018
Priority dateJun 7, 2017
Publication dateJan 11, 2022
Grant dateJan 11, 2022

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

An aluminum alloy pipe-shaped hollow material is produced by porthole extrusion. The aluminum alloy pipe-shaped hollow material includes an Al—Mg-based alloy containing Mg of 0.7 mass % or more and less than 2.5 mass %, and Ti of more than 0 mass % and 0.15 mass % or less, with the balance being Al and unavoidable impurities. A work hardening coefficient n-value is 0.25 or more and less than 0.43. The aluminum alloy pipe-shaped hollow material has an inner-surface ridged structure inside thereof, and an area ratio of the inner-surface ridged structure in a cross-section orthogonal to an extending direction of the aluminum alloy pipe-shaped hollow material is 1 to 30%. The present invention can provide an aluminum alloy pipe-shaped hollow material that is an aluminum alloy pipe-shaped hollow material of a 5000 series aluminum alloy produced by porthole extrusion and has excellent bending processability.

First claim

Opening claim text (preview).

The invention claimed is: 1. An aluminum alloy pipe-shaped hollow material produced by porthole extrusion, the aluminum alloy pipe-shaped hollow material comprising an Al—Mg-based alloy containing Mg of 0.7 mass % or more and less than 2.5 mass %, and Ti of more than 0 mass % and 0.15 mass % or less, with the balance being Al and unavoidable impurities, wherein a work hardening coefficient n-value is 0.25 or more and less than 0.43, and the aluminum alloy pipe-shaped hollow material having a pipe portion, a longitudinal axis, a hollow portion, and a ridged structure or partition portion formed on an inner surface of the pipe portion, the pipe portion being a base for the ridged structure or partition portion, the ridged structure or the partition portion having an area (B) measured in cross-section orthogonal to the longitudinal axis, the hollow portion having an area (A) defined by the formula π×(D I /2) 2 where D I is an inner diameter of the pipe-shaped hollow material measured in cross-section orthogonal to the longitudinal axis, an area ratio percentage of (B)/(A)×100 being between 1% and 30%. 2. The aluminum alloy pipe-shaped hollow material according to claim 1 , wherein the area ratio percentage is between 4% and 30%. 3. A piping material for a heat exchanger, the piping material being a product formed with the aluminum alloy pipe-shaped hollow material according to claim 1 .

Assignees

Inventors

Classifications

  • C22C21/06Primary

    with magnesium as the next major constituent · CPC title

  • from aluminium or aluminium alloys · CPC title

  • extruded · CPC title

  • Alloys based on aluminium · CPC title

  • Workpiece with longitudinal passageway or stopweld material [e.g., for tubular stock, etc.] · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US11220728B2 cover?
An aluminum alloy pipe-shaped hollow material is produced by porthole extrusion. The aluminum alloy pipe-shaped hollow material includes an Al—Mg-based alloy containing Mg of 0.7 mass % or more and less than 2.5 mass %, and Ti of more than 0 mass % and 0.15 mass % or less, with the balance being Al and unavoidable impurities. A work hardening coefficient n-value is 0.25 or more and less than 0.…
Who is the assignee on this patent?
Uacj Corp, Uacj Extrusion Corp
What technology area does this patent fall under?
Primary CPC classification C22C21/06. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue Jan 11 2022 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).