Poly(acrylated polyol) and method for making and using thereof as asphalt rubber modifiers, adhesive, fracking additives, or fracking fluids
US-10066051-B2 · Sep 4, 2018 · US
US11214714B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11214714-B2 |
| Application number | US-201916405697-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 7, 2019 |
| Priority date | May 8, 2018 |
| Publication date | Jan 4, 2022 |
| Grant date | Jan 4, 2022 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention relates to an adhesive comprising a thermoplastic polyacrylated glycerol polymer, water, and a cross linker that is reactive with the polyacrylated glycerol polymer. This adhesive is useful in the formation of cellulosic products including oriented strand board (OSB), particle board, oriented structural straw board, chipboard, plywood, laminated veneer lumber (LVL), pressed wood, glued laminated timber (glulam), cross-laminated timber (CLT), and other wood products. Methods of producing the adhesive and cellulosic products are also disclosed.
Opening claim text (preview).
What is claimed: 1. A composition comprising: a thermoplastic polyacrylated glycerol polymer prepared by first reacting acrylic reagent with glycerol to form acrylated glycerol monomers and then polymerizing the acrylated glycerol monomers, wherein the thermoplastic polyacrylated glycerol polymer is predominantly non-crosslinked; water; cellulosic particles or pieces; and a cross linker reactive with the polyacrylated glycerol polymer and mixed with the polyacrylated glycerol, the cellulosic particles or pieces, and the water. 2. The composition of claim 1 further comprising: an additive selected from the group consisting of inhibitors, initiators, and copolymers. 3. The composition of claim 1 , wherein the cross linker is selected from the group consisting of diisocyanates, anhydrides, multiply (meth)acrylated cross linkers, polyacids, and acid halides. 4. The composition of claim 3 , wherein the cross linker is polymeric methylene diphenyl diisocyanate. 5. The composition of claim 1 , wherein the thermoplastic polyacrylated glycerol polymer has a molecular weight ranging from 10 kDa to 10 MDa. 6. The composition of claim 1 , wherein the thermoplastic polyacrylated glycerol polymer has a molecular weight ranging from 500 kDa to 2 MDa. 7. The composition of claim 1 , wherein the thermoplastic polyacrylated glycerol polymer has a glass transition temperature (T g ) below 0° C. 8. The composition of claim 1 , wherein the cellulosic particles or pieces are wood particles or pieces.
Polyurethanes · CPC title
of esters containing halogen, nitrogen, sulfur or oxygen atoms in addition to the carboxy oxygen · CPC title
from particles · CPC title
from fibres · CPC title
Lignocellulosic material, e.g. wood, straw or bagasse {(manufacture of articles made from lignocellulosic material by dry processes B27N)} · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.