Rapid processing of laminar composite components
US-12180120-B2 · Dec 31, 2024 · US
US11078794B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11078794-B2 |
| Application number | US-201816043931-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 24, 2018 |
| Priority date | Feb 16, 2016 |
| Publication date | Aug 3, 2021 |
| Grant date | Aug 3, 2021 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Disclosed is a method of manufacturing an airfoil structure. The airfoil structure includes a plurality of airfoils, a support for supporting the airfoils, and a case for covering the airfoils. Each airfoil includes an airfoil body, and an airflow generator for producing induced airflow by generating plasma. The method includes a process of forming the airflow generator that includes a first electrode forming step of forming a first electrode on the airfoil body, a dielectric layer forming step of forming a dielectric layer on the airfoil body by forming ceramic powder into a film to cover the first electrode through room temperature impact consolidation, and a second electrode forming step of forming a second electrode on a surface of the dielectric layer, such that the second electrode is electrically connected to the first electrode, and an alternating-current voltage is applied to the second electrode.
Opening claim text (preview).
What is claimed is: 1. A method of manufacturing an airfoil structure to be used in a jet engine, the airfoil structure including a plurality of airfoils, a support for supporting the airfoils at their lower ends, and a case for covering upper ends of the airfoils, and each airfoil including an airfoil body formed extending in a longitudinal direction of the airfoil, and an airflow generator, provided to the airfoil body, for producing induced airflow by generating plasma, the method comprising a process of forming the airflow generator that includes: a first electrode forming step of forming a first electrode on the airfoil body; a dielectric layer forming step of forming a dielectric layer on the airfoil body by forming ceramic powder into a film to cover the first electrode through room temperature impact consolidation; and a second electrode forming step of forming a second electrode on a surface of the dielectric layer in a way that exposes the second electrode to an outside, such that the second electrode is electrically connected to the first electrode, wherein the second electrode is configured to receive alternating-current voltage, in the first electrode forming step, the first electrode is formed on an airfoil lateral surface of the airfoil body, the first electrode spanning from a trailing edge-side part of a negative pressure surface to a trailing edge-side part of a positive pressure surface via a leading edge, in the dielectric layer forming step, the dielectric layer is formed over an entirety pf the airfoil lateral surface of the airfoil body, and in the second electrode forming step, the second electrode is formed on the surface of the dielectric layer, which is opposite from the airfoil body, in the way that exposes the second electrode to the outside. 2. The method of manufacturing an airfoil structure according to claim 1 , wherein the process of forming the airflow generator further comprises a third electrode forming step of forming a third electrode on the surface of the dielectric layer in a way that exposes the third electrode to the outside, such that the third electrode is away from the second electrode, the third electrode is electrically connected to the first electrode, and the third electrode is configured to receive direct-current voltage. 3. The method of manufacturing an airfoil structure according to claim 1 , wherein in the dielectric layer forming step, the dielectric layer is formed using an aerosol deposition method. 4. The method of manufacturing an airfoil structure according to claim 1 , wherein a thickness of the dielectric layer is 100 μm.
Generating plasma {(nuclear fusion reactors G21B1/00; gas-filled discharge reactors H01J37/32)} · CPC title
Surface discharges, e.g. air flow control · CPC title
Layer deposition · CPC title
Blades · CPC title
comprising electromagnetic or electrostatic means for influencing the state of the fluid, e.g. for ionising the fluid or for generating a plasma · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.