Low density coated animal litter compositions
US-9986714-B2 · Jun 5, 2018 · US
US11076576B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11076576-B2 |
| Application number | US-201916460780-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 2, 2019 |
| Priority date | Jan 22, 2016 |
| Publication date | Aug 3, 2021 |
| Grant date | Aug 3, 2021 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A clumpable animal litter comprises composite particles of filler materials, such as limestone and sand, and sodium bentonite. The filler materials have a lower bulk density as compared to a granular mixture of the same percentage of filler and sodium bentonite clay and contain up to eighty-five percent less clay.
Opening claim text (preview).
The invention claimed is: 1. An animal litter comprising: composite particles of a filler material and sodium bentonite, the filler material and sodium bentonite being agglomerated together into the composite particles, wherein the filler material is present in an amount from about 60% to about 80% by weight of the composite particles and the sodium bentonite is present in an amount from about 20% to about 40% by weight of the composite particles; wherein the animal litter has a clump strength of at least 90% as measured by the Clump Strength Test Method. 2. The animal litter recited in claim 1 , wherein the filler material is present in an amount of about 70% by weight of the composite particles, and the sodium bentonite is present in an amount of about 30% by weight of the composite particles. 3. The animal litter recited in claim 1 , wherein the animal litter has a clump strength of at least 93%. 4. The animal litter recited in claim 1 , wherein the composite particles have a bulk density greater than 60 lb/ft 3 . 5. The animal litter recited in claim 1 , wherein the composite particles have a mean particle size from 0.4 mm to 2 mm. 6. The animal litter recited in claim 1 , wherein at least one of: (i) the filler material has a mean particle size of 0.5 mm or less; or (ii) the sodium bentonite has a mean particle size of 0.25 mm or less. 7. The animal litter recited in claim 1 , wherein the composite particles further comprise powered activated carbon. 8. The animal litter recited in claim 1 , wherein the filler material is limestone. 9. The animal litter recited in claim 1 , wherein the filler material comprises at least one of limestone, dolomite, calcite, calcium carbonates, sand, shale, gravel, or slate. 10. An animal litter comprising: composite particles of a filler material and sodium bentonite, the filler material and sodium bentonite being agglomerated together into the composite particles, wherein the filler material is present in an amount from about 50% to about 80% by weight of the composite particles and the sodium bentonite is present in an amount from about 20% to about 50% by weight of the composite particles; wherein the animal litter has a clump strength of at least 90% as measured by the Clump Strength Test Method. 11. The animal litter recited in claim 10 , wherein the composite particles further comprise powdered activated carbon. 12. The animal litter recited in claim 10 , wherein the filler material is limestone. 13. The animal litter recited in claim 10 , wherein the filler material comprises at least one of limestone, dolomite, calcite, calcium carbonates, sand, shale, gravel, or slate. 14. The animal litter recited in claim 10 , wherein the composite particles have a bulk density greater than 60 lb/ft 3 . 15. The animal litter recited in claim 10 , wherein the composite particles have a mean particle size from 0.4 mm to 2 mm. 16. The animal litter recited in claim 10 , wherein at least one of: (i) the filler material has a mean particle size of 0.5 mm or less; or (ii) the sodium bentonite has a mean particle size of 0.25 mm or less.
Granulating, agglomerating or aggregating · CPC title
comprising organic material · CPC title
Carbonates or bicarbonates, e.g. limestone, dolomite, aragonite · CPC title
Particle form · CPC title
comprising free carbon; comprising carbon obtained by carbonising processes · CPC title