Methods of packaging thin metal films to maintain their physical characteristics

US11059612B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-11059612-B2
Application numberUS-201615141983-A
CountryUS
Kind codeB2
Filing dateApr 29, 2016
Priority dateApr 30, 2015
Publication dateJul 13, 2021
Grant dateJul 13, 2021

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

The present disclosure is directed to the packaging of metal thin films deposited on polymeric substrates. The packaging method prevents deleterious change of surface energy/water contact angle as a function of time for metal thin films such as rolls, coils, sheets or strips of sputtered or vacuum deposited metal thin films. Methods and kits directed toward a unique packaging and storage scheme are also disclosed. This results in maintenance of the metal film's hydrophilicity and surface energy for extended periods of time.

First claim

Opening claim text (preview).

The invention claimed is: 1. A method of packaging a metal-coated substrate to maintain hydrophilicity and surface energy of a metal coating of the metal-coated substrate at as deposited levels, the method comprising: providing a metal-coated substrate in a form of a roll, wherein the roll consists of a polymeric substrate and a palladium metal coating directly applied to the substrate; placing disc separators on opposite sides of the roll, wherein the disc separators have a metalized polyester surface contacting the roll; and wrapping the metal-coated substrate and the disc separators in a polyester film. 2. The method of claim 1 , wherein a surface of the metal coating is hydrophilic in nature. 3. The method of claim 2 , wherein the metal coating has a water contact angle of 55 degrees or less after being wrapped in the polyester film for no less than 24 hours. 4. The method of claim 1 , wherein the metal coating shows no degradation of surface wettability after no less than 58 weeks; or wherein the metal coating shows no surface fouling after no less than 58 weeks; or wherein the metal coating shows no loss in surface energy after no less than 58 weeks. 5. The method of claim 1 , wherein the metal coating is in a form of a thin film on the substrate. 6. The method of claim 5 , wherein the thin film is formed through vacuum deposition. 7. The method of claim 1 , further comprising wrapping the substrate again to form a second wrapping layer, using a different covering material. 8. A method of packaging metal-coated products, each of the metal-coated products comprising a metal coating, to maintain hydrophilicity and surface energy of the metal coating of the metal-coated products at as deposited levels, the method comprising: providing metal-coated products each in a form of a roll, the roll consisting of a polymeric substrate and a palladium metal coating directly applied to the substrate; placing disc separators on opposite sides of the roll, wherein the disc separators have a metalized polyester surface contacting the roll; and covering each of the metal-coated products and the disk separators in a covering material selected from a group consisting of a polyester, a metalized polyester, an aluminum foil, and metalized polyethylene terephthalate (PET). 9. The method of claim 8 , wherein a surface of the metal coating is hydrophilic in nature. 10. The method of claim 9 , wherein the metal coating has a water contact angle of 65 degrees or less after being wrapped in the covering material for no less than 24 hours. 11. The method of claim 8 , wherein the metal coating shows no degradation of surface wettability after no less than 58 weeks; or wherein the metal coating shows no surface fouling after no less than 58 weeks; or wherein the metal coating shows no loss in surface energy after no less than 58 weeks. 12. The method of claim 8 , wherein the metal coating is in a form of a thin film on each of the products. 13. The method of claim 12 , wherein the thin film is formed through vacuum deposition. 14. A kit for packaging metal-coated products, the kit comprising: a polyester film; a plurality of disc separators having a metalized polyester surface and configured to separate a roll of a metal-coated substrate into a plurality of rolls, wherein each of the rolls consists of a polymeric substrate and a palladium metal coating directly applied to the substrate; at least one spacer, wherein the at least one spacer is a stiff corrugated polypropylene; a metal channel configured to support the plurality of rolls of the metal-coated substrate; and at least one board, wherein the at least one board includes a cutout through which the metal channel passes; wherein the plurality of rolls and the plurality of disc separators are wrapped by the polyester film.

Assignees

Inventors

Classifications

  • packaging rolled-up articles · CPC title

  • in sheets or blanks initially folded to form tubes · CPC title

  • Rigid or semi-rigid containers having bodies formed in one piece, e.g. by casting metallic material, by moulding plastics, by blowing vitreous material, by throwing ceramic material, by moulding pulped fibrous material or by deep-drawing operations performed on sheet material (with curved or partially-curved cross-section made by winding or bending paper B65D3/00; with polygonal cross-section formed by folding B65D5/00; specially constructed to be opened by cutting, piercing or tearing of wall portions B65D17/00; rigid pallets with side walls B65D19/02) · CPC title

  • Adaptations for preventing deterioration or decay of contents; Applications to the container or packaging material of food preservatives, fungicides, pesticides or animal repellants (with thermal insulation B65D81/38) · CPC title

  • Wrapping, e.g. partially or wholly enclosing, articles or quantities of material, in strips, sheets or blanks, of flexible material (bundling articles by applying narrow strips or bands of flexible material B65B13/00) · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US11059612B2 cover?
The present disclosure is directed to the packaging of metal thin films deposited on polymeric substrates. The packaging method prevents deleterious change of surface energy/water contact angle as a function of time for metal thin films such as rolls, coils, sheets or strips of sputtered or vacuum deposited metal thin films. Methods and kits directed toward a unique packaging and storage scheme…
Who is the assignee on this patent?
Materion Corp
What technology area does this patent fall under?
Primary CPC classification B65B11/58. Mapped technology areas include Operations & Transport.
When was this patent published?
Publication date Tue Jul 13 2021 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 1 related publication on this page (citations in our corpus or others sharing the same primary CPC).