Ni-Ir-based heat-resistant alloy and process for producing same
US-10094012-B2 · Oct 9, 2018 · US
US11053570B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11053570-B2 |
| Application number | US-201716469083-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 4, 2017 |
| Priority date | Dec 22, 2016 |
| Publication date | Jul 6, 2021 |
| Grant date | Jul 6, 2021 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention relates to a Ni-based heat-resistant alloy including Ir: 5.0 mass % or more and 50.0 mass % or less, Al: 1.0 mass % or more and 8.0 mass % or less, W: 5.0 mass % or more and 25.0 mass % or less, and balance Ni, having an L12-structured γ′ phase present in the matrix, and including at least one of Ru: 0.8 mass % or more and 5.0 mass % or less and Re: 0.8 mass % or more and 5.0 mass % or less. This Ni-based heat-resistant alloy has improved toughness over a conventional Ni-based heat-resistant alloy based on a Ni—Ir—Al—W-based alloy, and is also excellent in ambient-temperature strength.
Opening claim text (preview).
The invention claimed is: 1. A Ni-based heat-resistant alloy comprising Ir: 5.0 mass % or more and 35 mass % or less, Al: 1.0 mass % or more and 8.0 mass % or less, W: 5.0 mass % or more and 25.0 mass % or less, and balance Ni, having an L1 2 -structured γ′ phase present in the matrix, wherein the Ni-based heat-resistant alloy includes at least one of Ru: 0.8 mass % or more and 5.0 mass % or less and Re: 0.8 mass % or more and 5.0 mass % or less. 2. The Ni-based heat-resistant alloy according to claim 1 , comprising at least one addition element selected from the following: B: 0.001 mass % or more and 0.1 mass % or less Co: 5.0 mass % or more and 20.0 mass % or less Cr: 1.0 mass % or more and 25.0 mass % or less Ta: 1.0 mass % or more and 10.0 mass % or less Nb: 1.0 mass % or more and 5.0 mass % or less Ti: 1.0 mass % or more and 5.0 mass % or less V: 1.0 mass % or more and 5.0 mass % or less Mo: 1.0 mass % or more and 5.0 mass % or less. 3. The Ni-based heat-resistant alloy according to claim 1 , further comprising C: 0.001 mass % or more and 0.5 mass % or less. 4. The Ni-based heat-resistant alloy according to claim 2 , further comprising C: 0.001 mass % or more and 0.5 mass % or less.
based on nickel · CPC title
of nickel or cobalt or alloys based thereon · CPC title
with chromium · CPC title
with the maximum Cr content being at least 20% but less than 30% · CPC title
Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working (apparatus for mechanical working of metal B21, B23, B24) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.