A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a ferritic stainless steel excellent in oxidation resistance and thermal fatigue resistance. The ferritic stainless steel contains, in mass %, C: 0.020% or less, Si: more than 0.1% and 3.0% or less, Mn: 0.05 to 2.0%, P: 0.050% or less, S: 0.010% or less, Al: 0.3 to 6.0%, N: 0.020% or less, Cr: 12 to 30%, Nb: more than 0.3% and 1.0% or less, Ti: 0.01 to 0.5%, Mo: 0.3 to 6.0%, Co: 0.01 to 3.0%, and Ni: 0.02 to 1.0%, the balance being Fe and unavoidable impurities. Moreover, Si+Al>1.0%, Al—Mn>0%, and Nb—Ti>0% hold.
Opening claim text (preview).
The invention claimed is: 1. A ferritic stainless steel having a composition consisting of, in mass %, C: 0.020% or less, Si: more than 0.1% and 3.0% or less, Mn: 0.05 to 2.0%, P: 0.050% or less, S: 0.010% or less, Al: more than 2.0% to 6.0% or less, N: 0.020% or less, Cr: 14.0% to 30%, Nb: more than 0.3% and 1.0% or less, Ti: 0.01 to 0.5%, Mo: 0.3 to 6.0%, Co: 0.01 to 3.0%, Ni: 0.02 to 1.0%, and optionally one or two or more selected from B: 0.0002 to 0.0050%, Zr: 0.005 to 1.0%, V: 0.01 to 1.0%, W: 0.01 to 0.39%, Ca: 0.0002 to 0.0050% and Mg: 0.0002 to 0.0050%, with the balance being Fe and unavoidable impurities, wherein the ferritic stainless steel satisfies the following formulas (1) to (3): Si+Al>2.0% (1) Al—Mn>0% (2) Nb—Ti>0% (3), where the Si, Al, Mn, Nb, and Ti in the formulas (1) to (3) represent the contents, in mass %, of the respective elements.
during manufacturing of plates or strips (C21D8/12 takes precedence) · CPC title
Final recrystallisation annealing · CPC title
Very low carbon steels, i.e. having a carbon content of less than 0,01% · CPC title
with more than 1.5% by weight of manganese · CPC title