Nitrile group-containing highly saturated copolymer rubber composition and cross-linked rubber
US-2016297955-A1 · Oct 13, 2016 · US
US10964947B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10964947-B2 |
| Application number | US-201615736045-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jun 28, 2016 |
| Priority date | Jun 29, 2015 |
| Publication date | Mar 30, 2021 |
| Grant date | Mar 30, 2021 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a binder composition for a secondary battery electrode that, when used in production of a slurry composition for a secondary battery electrode, enables favorable dispersion of an electrode active material and a conductive material in high concentration while ensuring coatability. The binder composition for a secondary battery electrode contains a binder. The binder includes a copolymer that includes an alkylene structural unit and a nitrile group-containing monomer unit, and that has a Mooney viscosity (ML 1+4 , 100° C.) of at least 50 and not more than 200.
Opening claim text (preview).
The invention claimed is: 1. A binder composition for a secondary battery electrode comprising a binder and an organic solvent, wherein the binder includes a copolymer in a proportion of 60 mass % or more, the copolymer includes an alkylene structural unit and a nitrile group-containing monomer unit, and the copolymer has a Mooney viscosity ML 1+4 of at least 110 and not more than 200 as measured in accordance with JIS K 6300-1 at a temperature of 100° C. 2. The binder composition for a secondary battery electrode according to claim 1 , wherein the copolymer includes the alkylene structural unit in a proportion of at least 40 mass % and not more than 80 mass %. 3. The binder composition for a secondary battery electrode according to claim 1 , wherein the copolymer includes the nitrile group-containing monomer unit in a proportion of at least 10 mass % and not more than 55 mass %. 4. The binder composition for a secondary battery electrode according to claim 1 , wherein a proportion constituted by a hydrophilic group-containing monomer unit among all repeating units in the copolymer is 0 mass % or more and less than 0.05 mass %. 5. A slurry composition for a secondary battery electrode comprising: an electrode active material; a conductive material; and the binder composition for a secondary battery electrode according to claim 1 . 6. The slurry composition for a secondary battery electrode according to claim 5 , wherein the electrode active material includes a Ni-containing active material. 7. An electrode for a secondary battery comprising an electrode mixed material layer formed using the slurry composition for a secondary battery electrode according to claim 5 . 8. A secondary battery comprising the electrode for a secondary battery according to claim 7 . 9. The binder composition for a secondary battery electrode according to claim 1 , wherein the copolymer does not include a (meth)acrylic acid ester monomer unit and a hydrophilic group-containing monomer unit.
Reduction, e.g. hydrogenation · CPC title
Nitriles · CPC title
Homopolymers or copolymers of nitriles · CPC title
Use of inorganic substances as compounding ingredients · CPC title
of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx · CPC title