Method for producing hydrogen fluoride
US-11718523-B2 · Aug 8, 2023 · US
US10934166B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10934166-B2 |
| Application number | US-201515325361-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 2, 2015 |
| Priority date | Jul 11, 2014 |
| Publication date | Mar 2, 2021 |
| Grant date | Mar 2, 2021 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention provides a novel method for producing hydrogen fluoride which can suppress the occurrence of the pasty state over the whole process of producing hydrogen fluoride, reduce the problem of corrosion caused by sulfuric acid, and improve energy efficiency of the process. A method for producing hydrogen fluoride by reacting calcium fluoride and sulfuric acid comprises: (a) mixing and reacting calcium fluoride and sulfuric acid such that a mixture comprising calcium fluoride particles and sulfuric acid substantially maintains a form of particulate to obtain hydrogen fluoride while supplying sulfuric acid to the calcium fluoride particles at a flow rate of 0.002 to 1 mol/min relative to 1 mol of calcium fluoride to such an amount that a molar ratio of sulfuric acid/calcium fluoride is 0.9 to 1.1.
Opening claim text (preview).
The invention claimed is: 1. A method for producing hydrogen fluoride by reacting calcium fluoride and sulfuric acid, the method comprising: (b) mixing and reacting calcium fluoride and sulfuric acid such that a mixture comprising calcium fluoride particles and sulfuric acid is substantially maintained in a particulate form to obtain hydrogen fluoride, wherein sulfuric acid is supplied to the calcium fluoride particles at a flow rate of 0.002 to 0.07 mol/min relative to 1 mol of calcium fluoride at the start of the reaction in such an amount that a molar ratio of sulfuric acid/calcium fluoride is 0.9 to 1.1; and (c) mixing and reacting the intermediate product mixture with itself under a temperature condition higher than that in the step (b) to obtain hydrogen fluoride. 2. The method according to claim 1 , wherein the mixing is conducted in the step (b) by use of an apparatus having an attainment degree of mixing of 0.1 or more one minute after a start of the mixing. 3. The method according to claim 1 , wherein the step (b) is conducted at a temperature of 0 to 170° C. 4. The method according to claim 1 , wherein the step (c) is conducted at a temperature of 80 to 500° C. 5. The method according to claim 1 , wherein the calcium fluoride particles have a specific surface area of 0.5 to 30 m 2 /g.
Related publications grouped by family.
Answers are generated from the same data shown on this page.