Tissue paper
US-10618261-B2 · Apr 14, 2020 · US
US10844549B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10844549-B2 |
| Application number | US-201716338128-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 23, 2017 |
| Priority date | Sep 30, 2016 |
| Publication date | Nov 24, 2020 |
| Grant date | Nov 24, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
In one or more embodiments, the present invention is directed to a moisturizing tissue paper having excellent softness, smoothness, and strength. In various embodiments, the present invention provides a two-ply tissue paper containing a moisturizing agent having a basis weight per ply of 16.6 to 17.9 g/m2, a two-ply paper thickness of 143 to 159 μm, and containing a polyol, hyaluronic acid, a fatty acid ester-based compound, and a fatty acid amide-based compound.
Opening claim text (preview).
The invention claimed is: 1. A two-ply tissue paper comprising a moisturizing agent, wherein a basis weight per ply is 16.6 to 17.9 g/m 2 , a two-ply paper thickness is 143 to 159 μm, and all of a polyol, hyaluronic acid, a fatty acid ester-based compound, and a fatty acid amide-based compound are contained in the two-ply tissue paper, the content of a fatty acid ester-based compound is 0.10 to 0.50 parts by mass with respect to 100 parts by mass of a pulp fiber and the content of a fatty acid amide-based compound is 0.01 to 0.05 parts by mass with respect to 100 parts by mass of a pulp fiber, a wet tensile strength in CD is 36 cN/25 mm or more, and an evaluation value (T) determined by the following formula (1) is 97 or more, Evaluation value ( T )=(basis weight×two-ply paper thickness×moisture content)/(dry tensile strength in MD (machine direction)×dynamic friction coefficient average value measured by a pin-on-plate type friction test apparatus×friction coefficient maximum value measured by a pin-on-plate type friction test apparatus) (1).
Alcohols; Phenols; Ethers; Aldehydes; Ketones; Acetals; Ketals · CPC title
Carboxylic acids; Derivatives thereof · CPC title
Special paper not otherwise provided for, e.g. made by multi-step processes · CPC title
Paper towels; Toilet paper; Holders therefor · CPC title
Body washing or cleaning implements · CPC title