Thermoplastic Resin Composition for Laser Direct Structuring, and Molded Article Comprising Same
US-2020148849-A1 · May 14, 2020 · US
US10822505B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10822505-B2 |
| Application number | US-201615748412-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 13, 2016 |
| Priority date | Jul 28, 2015 |
| Publication date | Nov 3, 2020 |
| Grant date | Nov 3, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention relates to laser-markable polymers and coatings which are distinguished by the fact that they comprise tin/antimony oxide-coated spherical TiO2 particles of defined particle size as laser additive.
Opening claim text (preview).
The invention claimed is: 1. A method for the production of darkened laser-markings on a laser-markable polymer or on a laser-markable polymeric coating, which comprises: laser-treating the polymer or polymeric coating, which polymer or polymeric coating comprises a polymer and, in the polymer, a laser additive, which laser additive comprises spherical TiO 2 particles which are coated on the surface with an antimony-doped tin dioxide layer (Sn,Sb)O 2 and the TiO 2 particles have a number weighted particle size of <15 μm, measured at the D 95 by means of laser diffraction, and wherein, in the resulting polymer or polymeric coating, the laser-treating results in reducing the TiO 2 in the laser additive to Ti x O y , which results in a visibly darkened marking with a surface which is not roughened, where it was laser-treated. 2. The method of claim 1 , wherein the content of antimony in the tin dioxide layer is 0.1-60 mol %, based on the tin dioxide. 3. The method of claim 1 , wherein the laser additive has a number-weighted particle size of ≥0.05 μm, measured at the D 25 by means of laser diffraction. 4. The method of claim 1 , wherein the laser additive is employed in a concentration of 0.005 to 30% by weight, based on the polymer or polymeric coating. 5. The method of claim 1 , wherein the polymer is a thermoplastic, thermoset, elastomer or silicone. 6. The method of claim 1 , wherein the polymer additionally comprises one or more coloured pigments and/or dyes. 7. The method of claim 1 , wherein the content of antimony in the tin dioxide layer is 2-15 mol %, based on the tin dioxide. 8. A moulding composition, a product, a part or a film, which comprises a dark laser-marking on a polymer or polymeric coating thereof, which marking was produced by the method of claim 1 . 9. A powder coating, which comprises a dark laser-marking thereon, which marking was produced by the method of claim 1 .
Polypropene · CPC title
modified by treatment with other compounds · CPC title
characterised by the additives · CPC title
characterised by particle size or shape · CPC title
Coating · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.