Slurry recycling method, producing method of rare earth sintered magnet and slurry recycling apparatus

US10807167B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-10807167-B2
Application numberUS-201514817362-A
CountryUS
Kind codeB2
Filing dateAug 4, 2015
Priority dateMar 31, 2010
Publication dateOct 20, 2020
Grant dateOct 20, 2020

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

The present invention provides a producing method of a rare earth sintered magnet which is suitable as a producing method of a high performance rare earth sintered magnet which can reduce the number of steps for reusing defective molded bodies generated in a wet molding step of the rare earth sintered magnet, and which has a small content amount of oxygen. The invention also provides a slurry recycling method used for the producing method, and a slurry recycling apparatus. Each of the methods includes a crushing step of crushing, in mineral oil and/or synthetic fluid, a molded body in which slurry formed from alloy powder for a rare earth sintered magnet and mineral oil and/or synthetic fluid is wet molded in magnetic field, and recycling the crushed molded body into slurry.

First claim

Opening claim text (preview).

The invention claimed is: 1. A slurry recycling method comprising a crushing step of crushing, in mineral oil and/or synthetic fluid, a molded body obtained by wet molding, in magnetic field, slurry formed of alloy powder for a rare earth sintered magnet and mineral oil and/or synthetic fluid, and recycling the crushed molded body into slurry; and a storing step of storing, in mineral oil and/or synthetic fluid, the molded body before it is recycled into the slurry by the crushing step, wherein the crushing step includes a filtering step of removing foreign matters, said filtering step comprising: rotating a rotor in a cylindrical filter, wherein the cylindrical filter comprises annular plates spaced from each other at predetermined distances such that a gap is formed between opposed surfaces of the annular plates, to form a flow of slurry along an inner side wall of the cylindrical filter; and discharging the slurry out from the cylindrical filter by a centrifugal force. 2. The slurry recycling method according to claim 1 , wherein a particle diameter of the alloy powder for a rare earth sintered magnet in the recycled slurry which is recycled by the crushing step is not changed from a particle diameter of the alloy powder for the rare earth sintered magnet before it is recycled by the crushing step. 3. A producing method of a rare earth sintered magnet comprising a crushing step of crushing, in mineral oil and/or synthetic fluid, a molded body obtained by wet molding, in magnetic field, slurry formed of alloy powder for a rare earth sintered magnet and mineral oil and/or synthetic fluid, and recycling the crushed molded body into slurry; a storing step of storing, in mineral oil and/or synthetic fluid, the molded body before it is recycled into the slurry by the crushing step; and a recycled slurry sintering step of wet molding, in magnetic field, the recycled slurry which is recycled by the crushing step, and sintering an obtained molded body, wherein the crushing step includes a filtering step of removing foreign matters, said filtering step comprising: rotating a rotor in a cylindrical filter, wherein the cylindrical filter comprises annular plates spaced from each other at predetermined distances such that a gap is formed between opposed surfaces of the annular plates, to form a flow of slurry along an inner side wall of the cylindrical filter; and discharging the slurry out from the cylindrical filter by a centrifugal force. 4. A producing method of a rare earth sintered magnet comprising a crushing step of crushing, in mineral oil and/or synthetic fluid, a molded body obtained by wet molding, in magnetic field, slurry formed of alloy powder for a rare earth sintered magnet and mineral oil and/or synthetic fluid, and recycling the crushed molded body into slurry; a storing step of storing, in mineral oil and/or synthetic fluid, the molded body before it is recycled into the slurry by the crushing step; a mixing step of mixing, with each other, the recycled slurry which is recycled by the crushing step, and slurry including mineral oil and/or synthetic fluid and alloy powder for a rare earth sintered magnet which is obtained by roughly pulverizing and finely pulverizing raw material alloy obtained by melting raw material metal, thereby forming mixture slurry; and a sintering step of wet molding the mixture slurry in magnetic field, and sintering an obtained molded body, wherein the crushing step includes a filtering step of removing foreign matters, said filtering step comprising: rotating a rotor in a cylindrical filter, wherein the cylindrical filter comprises annular plates spaced from each other at predetermined distances such that a gap is formed between opposed surfaces of the annular plates, to form a flow of slurry along an inner side wall of the cylindrical filter; and discharging the slurry out from the cylindrical filter by a centrifugal force. 5. The producing method of a rare earth sintered magnet according to claim 3 , wherein a particle diameter of the alloy powder for a rare earth sintered magnet in the recycled slurry which is recycled by the crushing step is not changed from a particle diameter of the alloy powder for the rare earth sintered magnet before it is recycled by the crushing step. 6. The producing method of a rare earth sintered magnet according to claim 3 , wherein the storing step is carried out in the mineral oil and/or synthetic fluid accommodated in a storage container, and a space in the storage container which is not filled with the mineral oil and/or synthetic fluid is brought into inert gas atmosphere. 7. The producing method of a rare earth sintered magnet according to claim 4 , wherein a particle diameter of the alloy powder for a rare earth sintered magnet in the recycled slurry which is recycled by the crushing step is not changed from a particle diameter of the alloy powder for the rare earth sintered magnet before it is recycled by the crushing step. 8. A slurry recycling method comprising a crushing step of crushing, in mineral oil and/or synthetic fluid, a molded body obtained by wet molding, in magnetic field, slurry formed of alloy powder for a rare earth sintered magnet and mineral oil and/or synthetic fluid, and recycling the crushed molded body into slurry, wherein the crushing step includes: a roughly crushing step of the molded body, a finely crushing step of the roughly crushed molded body, and a returning step of the finely crushed molded body from the finely crushing step to the roughly crushing step, and, by circulating the slurry between the roughly crushing step and the finely crushing step, obtaining a slurry wherein a particle diameter of the alloy powder for a rare earth sintered magnet n the molded body before it is crushed and a particle diameter of the particles in the obtained slurry are the same.

Assignees

Inventors

Classifications

  • B22F8/00Primary

    Manufacture of articles from scrap or waste metal particles · CPC title

  • Reuse, recycling or recovery technologies · CPC title

  • from scrap particles · CPC title

  • containing cobalt · CPC title

  • within vertical containers {(B02C18/062, B02C18/065 take precedence)} · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US10807167B2 cover?
The present invention provides a producing method of a rare earth sintered magnet which is suitable as a producing method of a high performance rare earth sintered magnet which can reduce the number of steps for reusing defective molded bodies generated in a wet molding step of the rare earth sintered magnet, and which has a small content amount of oxygen. The invention also provides a slurry r…
Who is the assignee on this patent?
Hitachi Metals Ltd
What technology area does this patent fall under?
Primary CPC classification B22F8/00. Mapped technology areas include Operations & Transport.
When was this patent published?
Publication date Tue Oct 20 2020 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?