Hot blow forming method for aluminum alloy sheet

US10807142B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-10807142-B2
Application numberUS-201515528941-A
CountryUS
Kind codeB2
Filing dateApr 21, 2015
Priority dateNov 24, 2014
Publication dateOct 20, 2020
Grant dateOct 20, 2020

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A hot blow forming method for the aluminum alloy sheet carries out a hot blow forming to an aluminum alloy sheet using a first metal mold being a female mold for forming having a protruding surface portion on an inside surface thereof and a second metal mold for gas introduction. Immediately prior to the hot blow forming, a temperature (T1) of the aluminum alloy sheet and a temperature (T2) of the first metal mold satisfy a relation (T1)-(T2)≥30° C. and the temperature (T2) is equal to or higher than 400° C. In the hot blow forming, the aluminum alloy sheet is made to be brought into contact with at least a part of the protruding surface portion of the first metal mold within 30 seconds from a start of the gas introduction from the second metal mold.

First claim

Opening claim text (preview).

The invention claimed is: 1. A hot blow forming method for an aluminum alloy sheet comprising: carrying out hot blow forming for the aluminum alloy sheet using a first metal mold, which is a female mold for forming having a protruding surface portion on an inside surface thereof, and a second metal mold for gas introduction, wherein, immediately prior to the hot blow forming, a temperature (T1) of the aluminum alloy sheet and a temperature (T2) of the first metal mold satisfy a relation (T1)-(T2)≥30° C., and the temperature (T2) is equal to or more than 400° C., and wherein, in the hot blow forming, the aluminum alloy sheet is brought into contact with at least a part of the protruding surface portion of the first metal mold within 30 seconds from a start of gas introduction from the second metal mold. 2. The hot blow forming method for an aluminum alloy sheet according to claim 1 , wherein a temperature (T3) of the second metal mold immediately prior to the hot blow forming is lower than a melting point of the aluminum alloy sheet and is equal to or higher than the temperature (T1). 3. The hot blow forming method for an aluminum alloy sheet according to claim 1 , wherein the aluminum alloy sheet is comprised of, by mass %, 1.1 to 6.5% Mg, 0.01 to 0.3% Fe, and a balance Al and inevitable impurities, and wherein the temperature (T1) is equal to or lower than 550° C. 4. The hot blow forming method for an aluminum alloy sheet according to claim 1 , wherein the aluminum alloy sheet is comprised of, by mass %, 0.2 to 2.0% Si, 0.2 to 1.5% Mg, 0.01 to 0.3% Fe, and a balance Al and inevitable impurities, and wherein the temperature (T1) is equal to or lower than 550° C.

Assignees

Inventors

Classifications

  • C22C21/02Primary

    with silicon as the next major constituent · CPC title

  • B21D26/021Primary

    Deforming sheet bodies · CPC title

  • Process control or regulation for heat treatments · CPC title

  • with silicon · CPC title

  • by applying fluid pressure · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US10807142B2 cover?
A hot blow forming method for the aluminum alloy sheet carries out a hot blow forming to an aluminum alloy sheet using a first metal mold being a female mold for forming having a protruding surface portion on an inside surface thereof and a second metal mold for gas introduction. Immediately prior to the hot blow forming, a temperature (T1) of the aluminum alloy sheet and a temperature (T2) of …
Who is the assignee on this patent?
Uacj Corp
What technology area does this patent fall under?
Primary CPC classification C22C21/02. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue Oct 20 2020 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 6 related publications on this page (citations in our corpus or others sharing the same primary CPC).