Spherical silica particles and resin composition using same
US-2024417544-A1 · Dec 19, 2024 · US
US10745545B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10745545-B2 |
| Application number | US-201615577058-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 11, 2016 |
| Priority date | Jun 3, 2015 |
| Publication date | Aug 18, 2020 |
| Grant date | Aug 18, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
This disclosure is to provide a method of manufacturing a rubber composition comprising kneading a rubber composition that includes 100 parts by mass (pbm) of a rubber component (A) including 50 mass % or more of natural rubber, 5-50 pbm of at least one kind of thermoplastic resin (B) selected from among C5-based resins, C5-C9-based resins, C9-based resins, terpene-based resins, terpene-aromatic compound-based resins, rosin-based resins, dicyclopentadiene resins, and alkylphenol-based resins; 20-120 pbm of a filler (C) including silica; at least one kind of vulcanization accelerator (D) selected from among guanidines, sulfenamides, thiazoles, thiourea and diethyl thiourea; a silane coupling agent (E); and a vulcanizing agent (F). The kneading comprises a kneading stage A for kneading components (A)-(C), part or all of component (D), and 2 pbm or more of component (E), and a kneading stage B for kneading component (F) with a kneaded product of the kneading stage A.
Opening claim text (preview).
The invention claimed is: 1. A method of manufacturing a rubber composition, the method comprising kneading a rubber composition, wherein the rubber composition comprises a rubber component (A) including 50 mass % or more of natural rubber; at least one kind of thermoplastic resin (B) selected from the group consisting of terpene-based resins, terpene-aromatic compound-based resins, rosin-based resins, dicyclopentadiene resins, and alkylphenol-based resins, 5 parts by mass to 50 parts by mass of the at least one kind of thermoplastic resin (B) per 100 parts by mass of the rubber component being included; a filler (C) including silica, 20 parts by mass to 120 parts by mass of the filler (C) per 100 parts by mass of the rubber component being included; a vulcanization accelerator (D) as a combination of at least one selected from the group consisting of guanidines, sulfenamides, and thiazoles with diethyl thiourea; a silane coupling agent (E); and a vulcanizing agent (F), and the kneading comprises: a kneading stage A for kneading the rubber component (A), the thermoplastic resin (B), the filler (C), diethyl thiourea of the vulcanization accelerator (D), and 2 parts by mass or more of the silane coupling agent (E) per 100 parts by mass of the rubber component, and a kneading stage B, after the kneading stage A, for kneading at least one selected from the group consisting of guanidines, sulfenamides, and thiazoles of the vulcanization accelerator (D), and the vulcanizing agent (F) with a kneaded product prepared by the kneading in the kneading stage A. 2. The method of manufacturing a rubber composition of claim 1 , wherein 5 mass % or more to less than 50 mass % of styrene-butadiene copolymer rubber is included in the rubber component (A). 3. The method of manufacturing a rubber composition of claim 1 , wherein a content of the silica in the filler (C) is 50 mass % to 100 mass %. 4. The method of manufacturing a rubber composition of claim 3 , wherein a content of the silica in the filler (C) is 90 mass % or more. 5. The method of manufacturing a rubber composition of claim 2 , wherein a content of the silica in the filler (C) is 50 mass % to 100 mass %. 6. The method of manufacturing a rubber composition of claim 5 , wherein a content of the silica in the filler (C) is 90 mass % or more.
Silica · CPC title
Fillers or reinforcements {, e.g. fibres} · CPC title
measuring properties of the mixture, e.g. temperature, density (B29B7/283 takes precedence) · CPC title
having a casing closely surrounding the rotors, e.g. of Banbury type (with single shaft B29B7/125) · CPC title
for mixing in batches · CPC title