Rubber composition, rubber roller, and image forming apparatus
US-2019225777-A1 · Jul 25, 2019 · US
US10738136B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10738136-B2 |
| Application number | US-201716079267-A |
| Country | US |
| Kind code | B2 |
| Filing date | Feb 22, 2017 |
| Priority date | Feb 29, 2016 |
| Publication date | Aug 11, 2020 |
| Grant date | Aug 11, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of production of a polyether rubber containing unit expressed by the following general formula (1) in 0.1 mol % or more and less than 30 mol % obtained by reacting a polyether rubber containing epihalohydrin monomer unit in 0.1 mol % or more and a nitrogen atom-containing aromatic heterocyclic compound by kneading in the presence of an acid acceptor containing at least a hydrotalcite having a nitrogen adsorption specific surface area as measured by a BET method of 10 m 2 /g or more is provided. wherein, in the above general formula (1), A + is a group containing a cationic nitrogen-containing aromatic heterocyclic ring, and is bonded with a carbon atom at the “2” position shown in the above general formula (1) through a nitrogen atom constituting the cationic nitrogen-containing aromatic heterocyclic ring, and X − is any counter anion.
Opening claim text (preview).
The invention claimed is: 1. A method of production of a polyether rubber containing unit expressed by the following general formula (1) in 0.1 mol % or more and less than 30 mol % comprising: reacting a polyether rubber containing epihalohydrin monomer unit in 0.1 mol % or more and a nitrogen atom-containing aromatic heterocyclic compound by kneading in the presence of an acid acceptor containing at least a hydrotalcite having a nitrogen adsorption specific surface area as measured by a BET method of 14 m 2 /g or more so as to substitute at least part of halogen atom constituting the epihalohydrin monomer unit with a group containing a cationic nitrogen-containing aromatic heterocyclic ring: wherein, in the above general formula (1), A + is a group containing a cationic nitrogen-containing aromatic heterocyclic ring, where the group containing a cationic nitrogen-containing aromatic heterocyclic ring is bonded with a carbon atom at the “2” position shown in the above general formula (1) through a nitrogen atom constituting the cationic nitrogen-containing aromatic heterocyclic ring, and X − is any counter anion. 2. The method of production of a polyether rubber according to claim 1 , wherein an amount of the hydrotalcite to be used is 0.1 to 15 parts by weight with respect to 100 parts by weight of the polyether rubber containing epihalohydrin monomer unit in 0.1 mol % or more. 3. The method of production of a polyether rubber according to claim 1 , wherein the hydrotalcite contains at least Mg and Al. 4. The method of production of a polyether rubber according to claim 1 , wherein the nitrogen atom-containing aromatic heterocyclic compound is a five-membered heterocyclic compound or a six-membered heterocyclic compound. 5. The method of production of a polyether rubber according to claim 1 , wherein, further, an oxide, hydroxide, and/or carbonate of at least one of magnesium, calcium, and barium are used as the acid acceptor in a proportion of 0.1 to 5 parts by weight with respect to 100 parts by weight of the polyether rubber containing epihalohydrin monomer unit in 0.1 mol % or more. 6. The method of production of a polyether rubber according to claim 1 , wherein, further, magnesium oxide is used as the acid acceptor in a proportion of 0.1 to 2 parts by weight with respect to 100 parts by weight of the polyether rubber containing epihalohydrin monomer unit in 0.1 mol % or more.
Carbonates; Bicarbonates · CPC title
heterocyclic · CPC title
Magnesia, i.e. magnesium oxide · CPC title
Epihalohydrins · CPC title
Magnesium carbonate · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.