Odor adsorbent
US-2016074550-A1 · Mar 17, 2016 · US
US10731024B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10731024-B2 |
| Application number | US-201715831349-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 4, 2017 |
| Priority date | Mar 31, 2017 |
| Publication date | Aug 4, 2020 |
| Grant date | Aug 4, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A superabsorbent polymer includes polymer particles, surface cross-linking agents and particles made of silicon-containing inorganic salt. The polymer particles have cross-linking inside the polymer particles. The surface cross-linking agents are covalently bound to the surface of the polymer particles so as to constitute a surface cross-linked region at the surface of each said resin particle, and the particles made of silicon-containing inorganic salt cover the surface of the polymer particles.
Opening claim text (preview).
What is claimed is: 1. A method for producing a superabsorbent polymer, comprising: providing an acid-based monomer aqueous solution and performing a radical polymerization reaction to obtain a superabsorbent polymer having an internal crosslinking structure; cutting said superabsorbent polymer to obtain a plurality of superabsorbent polymer particles; adding a surface cross-linking agent to a surface of each of said superabsorbent polymer particles and performing a heat treatment so as to constitute a surface cross-linked region at the surface of each said resin particle; and coating said surface of each of said superabsorbent polymer particles with an aqueous solution having silicon-containing inorganic salt-containing particles, wherein a pH value of said aqueous solution having said silicon-containing inorganic salt-containing particles is between 4 and 6.5. 2. The method for producing a superabsorbent polymer of claim 1 , wherein a weight percentage of said aqueous solution having said silicon-containing inorganic salt-containing particles to said superabsorbent polymer particles is between 0.5% to 20%. 3. The method for producing a superabsorbent polymer of claim 1 , wherein a weight ratio of alumina to silicon oxide in said silicon-containing inorganic salt-containing particles is between 0.7 and 0.95. 4. The method for producing a superabsorbent polymer of claim 1 , wherein each of said silicon-containing inorganic salt-containing particles has a particle size between 1 and 10 μm. 5. The method for producing a superabsorbent polymer of claim 1 , wherein each of said silicon-containing inorganic salt-containing particles is composed of kaolinite.
containing inorganic materials · CPC title
Silicon-containing compounds · CPC title
Powdering or granulating · CPC title
Acrylic acid; Methacrylic acid; Metal salts or ammonium salts thereof · CPC title