Tire sidewall composition and tire sidewall
US-2024392114-A1 · Nov 28, 2024 · US
US10723176B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10723176-B2 |
| Application number | US-201615556285-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 3, 2016 |
| Priority date | Mar 6, 2015 |
| Publication date | Jul 28, 2020 |
| Grant date | Jul 28, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present technology provides a rubber composition for sidewalls containing, a diene rubber, from 10 to 120 parts by mass of a carbon black, and from 3 to 30 parts by mass of an acid-modified polyolefin having a melting point of from 100 to 150° C. per 100 parts by mass of the diene rubber, a main chain of the acid-modified polyolefin being a homopolymer of an olefin; and a pneumatic tire using the same in sidewalls thereof.
Opening claim text (preview).
The invention claimed is: 1. A rubber composition for sidewalls comprising: a diene rubber containing natural rubber and butadiene rubber, a content of the butadiene rubber being not less than 30 parts by mass per 100 parts by mass of the diene rubber and a total content of both of the natural rubber and the butadiene rubber being greater than 50 mass % of the diene rubber; from 10 to 120 parts by mass of a carbon black; and from 3 to 30 parts by mass of an acid-modified polyolefin having a melting point of from 100 to 150° C. per 100 parts by mass of the diene rubber, a main chain of the acid-modified polyolefin being a homopolymer of an olefin. 2. The rubber composition for sidewalls according to claim 1 , wherein a main chain of the acid-modified polyolefin is a polyethylene, polypropylene, or polybutene. 3. The rubber composition for sidewalls according to claim 1 , wherein the acid-modified polyolefin is a polyolefin modified with a carboxylic acid or an acid anhydride. 4. The rubber composition for sidewalls according to claim 1 , wherein a melt mass flow rate of the acid-modified polyolefin at 190° C. is from 1.0 to 8.0 g/10 min. 5. A pneumatic tire using the rubber composition for sidewalls according to claim 1 as a sidewall. 6. The rubber composition for sidewalls according to claim 2 , wherein the acid-modified polyolefin is a polyolefin modified with a carboxylic acid or an acid anhydride. 7. The rubber composition for sidewalls according to claim 6 , wherein a melt mass flow rate of the acid-modified polyolefin at 190° C. is from 1.0 to 8.0 g/10 min. 8. A pneumatic tire using the rubber composition for sidewalls according to claim 7 as a sidewall.
Tyres characterised by the chemical composition or the physical arrangement or mixture of the composition · CPC title
Waxes · CPC title
Compositions of oils, fats or waxes; Compositions of derivatives thereof · CPC title
Carbon · CPC title
modified by chemical after-treatment (saponified copolymers C08L23/0861; unsaturated acid salts C08L23/0876) · CPC title