Nickel-cobalt composite hydroxide and process for manufacturing same
US-2015364759-A1 · Dec 17, 2015 · US
US10689262B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10689262-B2 |
| Application number | US-201716302834-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jun 12, 2017 |
| Priority date | Jun 14, 2016 |
| Publication date | Jun 23, 2020 |
| Grant date | Jun 23, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for producing a nickel-containing hydroxide is provided that includes a particle growth step of promoting growth of nickel-containing hydroxide particles by neutralization crystallization in an aqueous solution accommodated in an agitation tank. In the particle growth step, an averaged value of the maximum accelerations of the flows of streamlines for the aqueous solution is greater than 600 m/s 2 .
Opening claim text (preview).
The invention claimed is: 1. A method for producing a nickel-containing hydroxide, the method comprising: a particle growth step of promoting growth of nickel-containing hydroxide particles by neutralization crystallization in an aqueous solution accommodated in an agitation tank; wherein in the particle growth step, an averaged value of maximum accelerations of flows of streamlines for the aqueous solution is greater than 600 m/s 2 . 2. The method for producing a nickel-containing hydroxide according to claim 1 , wherein the nickel-containing hydroxide is produced so as to contain Ni, Co, and Al at an amount ratio of Ni:Co:Al=(1-x-y):x:y, where 0≤x≤0.3 and 0.005≤y≤0.15. 3. The method for producing a nickel-containing hydroxide according to claim 1 , wherein the nickel-containing hydroxide is produced so as to contain Ni, Co, Mn, and M, where M denotes at least one additional element selected from a group consisting of Ti, V, Cr, Zr, Nb, Mo, Hf, Ta, and W, at an amount ratio of Ni:Co:Mn:M=x:y:z:t, where x+y+z+t=1, 0.1≤x≤0.7, 0.1≤y≤0.5, 0.1≤z≤0.8, and 0≤t≤0.02.