Flux for submerged arc welding
US-2016175993-A1 · Jun 23, 2016 · US
US10688602B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10688602-B2 |
| Application number | US-201715645394-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 10, 2017 |
| Priority date | Jul 13, 2016 |
| Publication date | Jun 23, 2020 |
| Grant date | Jun 23, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A submerged arc welding process using welding wire containing, based on the total mass of the welding wire, Ni: 50% or more by mass, Cr: 14.5% to 16.5% by mass, Mo: 15.0% to 17.0% by mass, W: 3.0% to 4.5% by mass, Fe: 4.0% to 7.0% by mass, and C, Si, Mn, P, S, Cu, V, Co, and Al: a predetermined amount or less, and a bonded flux containing, based on the total mass of the bonded flux, Al 2 O 3 : 35% to 55% by mass, SiO 2 : 5% to 25% by mass, CaO: 2% to 10% by mass, CaF 2 : 25% to 45% by mass, and Na 2 O: 2% to 4% by mass.
Opening claim text (preview).
What is claimed is: 1. A submerged arc welding process using a welding wire and a bonded flux in combination, wherein the welding wire contains, based on a total mass of the welding wire, Ni: 50% or more by mass, Cr: 14.5% to 16.5% by mass, Mo: 15.0% to 17.0% by mass, W: 3.0% to 4.5% by mass, Fe: 4.0% to 7.0% by mass, C: 0.02% or less by mass (excluding 0% by mass), Si: 0.08% or less by mass (excluding 0% by mass), Mn: 1.0% or less by mass (excluding 0% by mass), P: 0.04% or less by mass (excluding 0% by mass), S: 0.03% or less by mass (excluding 0% by mass), Cu: 0.5% or less by mass (excluding 0% by mass), V: 0.35% or less by mass (excluding 0% by mass), Co: 2.5% or less by mass (excluding 0% by mass), and Al: 0.1% or less by mass (excluding 0% by mass), and the bonded flux contains, based on a total mass of the bonded flux, Al 2 O 3 : 35% to 55% by mass, SiO 2 : 5% to 25% by mass, CaO: 2% to 10% by mass, CaF 2 : 25% to 45% by mass, and Na 2 O: 2% to 4% by mass, wherein the bonded flux is substantially free of Al and Si. 2. The submerged arc welding process according to claim 1 , wherein the bonded flux is substantially free of carbonates. 3. The submerged arc welding process according to claim 2 , applied to welding of steel for cryogenic liquid storage. 4. The submerged arc welding process according to claim 1 , applied to welding of steel for cryogenic liquid storage.
Ni as the principal constituent · CPC title
Submerged-arc welding · CPC title
with Cr as the next major constituent · CPC title
Alumina or aluminates · CPC title
Fluorides · CPC title