Soft magnetic alloy, wireless power transmitting apparatus and wireless power receiving apparatus comprising the same
US-2015325365-A1 · Nov 12, 2015 · US
US10594141B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10594141-B2 |
| Application number | US-201514943286-A |
| Country | US |
| Kind code | B2 |
| Filing date | Nov 17, 2015 |
| Priority date | Nov 17, 2014 |
| Publication date | Mar 17, 2020 |
| Grant date | Mar 17, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention relates to a soft magnetic alloy and, more specifically, to a soft magnetic alloy used in electric transformers, pulse generators, compressions, electric chokes, energy-accumulating inductors, magnetic sensors, or the like, and a wireless power transmitting apparatus and wireless power receiving apparatus including the soft magnetic alloy.
Opening claim text (preview).
What is claimed is: 1. A soft magnetic alloy, consisting of a composition expressed by a formula: Fe a X b Y c , wherein X represents a first metalloid element, Y represents a second metalloid element and a content of the first and second metalloid elements (X+Y) is in the range of 9 to 15.5 at %, and wherein the composition consists of Fe, X, and Y, wherein the first metalloid element is B and the second metalloid element is Si, wherein a is in the range of 84.5 to 91.0 at %, b is in the range of 5.3 to 9.0 at %, and c is in the range of 3.8 to 6.5 at %, and wherein B/Si, which is a content ratio of B and Si, is 1.4 so that the amount of saturated magnetic induction of the soft magnetic alloy is in the range of 1.78˜1.95 T, a resistivity of the soft magnetic alloy is in the range of 45.7˜52.6μΩ·cm, and a saturated Magnetization is in the range of 182.2˜199.2 emu/g so as to be used at frequency band in the range of 110 kHz˜250 kHz. 2. The soft magnetic alloy of claim 1 , wherein a content of the first and second metalloid elements (X+Y) is in a range of from 12.65 at % to 15.5 at %. 3. The soft magnetic alloy of claim 1 , wherein the soft magnetic alloy is thermally treated by annealing at a temperature between 350° C. and 400° C.
containing silicon · CPC title
containing aluminium · CPC title
Inductive couplings {(for wireless supply or distribution of electric power using inductive coupling H02J50/10)} · CPC title
containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60 · CPC title
using inductive coupling · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.