Component fabrication method including a modified burnishing step

US10564606B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-10564606-B2
Application numberUS-201615162763-A
CountryUS
Kind codeB2
Filing dateMay 24, 2016
Priority dateJun 16, 2015
Publication dateFeb 18, 2020
Grant dateFeb 18, 2020

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

The invention relates to a fabrication method for a part intended to be welded comprising a burnishing step for forming a perpendicular wall with respect to the surface undergoing burnishing intended to improve the flatness of the face to be welded.

First claim

Opening claim text (preview).

What is claimed is: 1. A method for fabrication of a timepiece component comprising: selecting a metal bar; forming at least one diameter portion including a substantially vertical surface and a substantially horizontal surface based on a profile turning of the metal bar; forming a first metal part based on a burnishing of the metal bar, the burnished metal bar having increased hardness and improved surface state than the metal bar, wherein a burnisher is moved along the substantially vertical surface of the at least one diameter portion until the burnisher is in contact with the substantially horizontal surface of the at least one diameter portion, and the substantially horizontal surface of the at least one diameter portion is polished when the burnisher is moved away from the substantially vertical surface of the at least one diameter portion; mounting a surface of the first metal part on a surface of a second part; and welding, by laser electromagnetic radiation, the surface of the metal first part mounted on the surface of the second part, the first metal part being secured to the second part. 2. The method according to claim 1 , wherein the second part includes silicon or ceramic. 3. The method according to claim 2 , wherein the second part further includes at least a partial coating of metal, silicon oxide, silicon nitride, silicon carbide or an allotrope of carbon. 4. The method according to claim 1 , wherein the first metal part is made from a metal includes ail iron alloy, a copper alloy, nickel or an alloy thereof, titanium or an alloy thereof, gold or an alloy thereof, silver or an alloy thereof platinum or an alloy thereof ruthenium or an alloy thereof, rhodium or an alloy thereof, or palladium or art alloy thereof. 5. The method according to claim 1 , wherein a side face of the burnisher is configured to polish the substantially horizontal surface of the at least one diameter portion. 6. The method according to claim 1 , wherein the at least one diameter portion is configured to receive a balance spring, a balance Wheel, and a table-roller of the timepiece component. 7. The method according to claim 1 , wherein the at least one diameter portion further includes a cylindrical shaft and a shoulder, a lower portion of the cylindrical shaft being edged with the shoulder. 8. The method according to claim 1 , wherein a side face of the burnisher is configured to polish the substantially horizontal surface of the at least one diameter portion. 9. The method according to claim 1 , wherein the first metal part is a balance staff. 10. The method according to claim 1 , wherein the second part is a collet.

Assignees

Inventors

Classifications

  • Component parts or constructional details, e.g. collet, stud {, virole or piton} · CPC title

  • G04B13/02Primary

    Wheels; Pinions; Spindles; Pivots (bearings G04B31/00 {; chain wheels, spindles for chain wheels, also chains and driving weights G04B1/08}) · CPC title

  • Manufacture of the spiral spring (locking of the spiral spring by the regulating lever G04B18/026; spiral spring with temperature compensation G04B17/227; fixation of the spiral spring on the collet G04B17/32; mainspring G04B1/14) · CPC title

  • Component parts or constructional details, e.g. construction of the lever or the escape wheel {(assembly and manufacture of the spring G04B1/145; assembly and manufacture of components, e.g. pinions, spindles G04B13/02; lubrication of clockwork bearings G04B31/008; oils for clockwork bearings in general G04B31/08)} · CPC title

  • Dissimilar materials · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US10564606B2 cover?
The invention relates to a fabrication method for a part intended to be welded comprising a burnishing step for forming a perpendicular wall with respect to the surface undergoing burnishing intended to improve the flatness of the face to be welded.
Who is the assignee on this patent?
Nivarox Sa
What technology area does this patent fall under?
Primary CPC classification G04B13/02. Mapped technology areas include Physics.
When was this patent published?
Publication date Tue Feb 18 2020 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.