Porous cellulose body and method for producing same
US-2015093560-A1 · Apr 2, 2015 · US
US10556197B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10556197-B2 |
| Application number | US-201515743866-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 3, 2015 |
| Priority date | Aug 3, 2015 |
| Publication date | Feb 11, 2020 |
| Grant date | Feb 11, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for manufacturing a filter medium for an air filter having improved particle collection performance using cellulose nanofibers. The method for manufacturing a filter medium for an air filter comprises: causing a mixed solution containing cellulose nanofibers and a dispersion medium to adhere to an air-permeable support; and subsequently freeze-drying the resulting product, in which a number average fiber diameter of the cellulose nanofibers is 1 to 50 nm, the dispersion medium is a mixed dispersion medium of water and a water-soluble organic solvent, and a solid content concentration of the cellulose nanofibers in the mixed solution is 0.001 to 0.150% by mass.
Opening claim text (preview).
The invention claimed is: 1. A method for manufacturing a filter medium for an air filter, the method comprising: causing a mixed solution containing cellulose nanofibers and a dispersion medium to adhere to an air-permeable support; and subsequently freeze-drying the resulting product, wherein the cellulose nanofibers have an average fiber diameter that is in a range of 1 to 50 nm, wherein the dispersion medium is a mixed dispersion medium of water and a water-soluble organic solvent, and wherein the cellulose nanofibers in the mixed solution have a solid content concentration in a range of 0.001 to 0.150% by mass wherein the cellulose nanofibers have an adhesion amount ratio with respect to the air-permeable support in a range of 0.001 to 0.200% by mass. 2. The method for manufacturing a filter medium for an air filter according to claim 1 , the method further comprising: setting an ambient temperature of the mixed solution adhered to the air-permeable support to a temperature equal to or lower than a melting point of the mixed solution in the freeze-drying. 3. The method for manufacturing a filter medium for an air filter according to claim 1 , wherein the filter medium has a PF value that is higher than a PF value of a support by 0.5 or more when a surface wind speed is 5.3 cm/sec and a target particle diameter is 0.10 to 0.15 μm.
the material being cellulose or derivatives thereof ({cork or peat B01D39/1646} ; making filter paper D21F11/14) · CPC title
comprising nanofibres · CPC title
the material being filamentary or fibrous · CPC title
After-treatment (C08J9/22 takes precedence) · CPC title
Fibre diameter · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.