Rubber composition and tire

US10550248B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-10550248-B2
Application numberUS-201414913638-A
CountryUS
Kind codeB2
Filing dateAug 11, 2014
Priority dateAug 23, 2013
Publication dateFeb 4, 2020
Grant dateFeb 4, 2020

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

The present invention provides a rubber composition capable of producing a rubber molded article that is excellent in rolling resistance performance, steering stability, mechanical strength and abrasion resistance, and a tire obtained by using the rubber composition in at least a part thereof. The present invention relates to a rubber composition including (A) a rubber component including at least one rubber selected from the group consisting of a synthetic rubber and a natural rubber, (B) silica and (C) a modified polymer of farnesene obtained by introducing a functional group into a polymer of farnesene, in which a content of the silica (B) in the rubber composition is from 20 to 150 parts by mass on the basis of 100 parts by mass of the rubber component (A), and a content of the modified farnesene polymer (C) in the rubber composition is from 2 to 10 parts by mass on the basis of 100 parts by mass of the silica (B).

First claim

Opening claim text (preview).

The invention claimed is: 1. A rubber composition comprising (A) a rubber component comprising at least one rubber selected from the group consisting of a styrene-butadiene rubber, a butadiene rubber, an isoprene rubber, a butyl rubber, a halogenated butyl rubber, an ethylene propylene diene rubber, a butadiene acrylonitrile copolymer rubber, a chloroprene rubber and a natural rubber, (B) silica and (C) a modified polymer consisting of farnesene units, optionally other monomer units, and a functional group on the modified polymer, wherein the functional group is selected from the group consisting of an amino group, an ammonium group, an amide group, an imino group, an imidazole group, a urea group, an alkoxysilyl group, a silanol group, a hydroxy group, an epoxy group, an ether group, a carboxy group, a carbonyl group, a carboxylate group, a sulfonic group, a sulfonate group, a phosphoric group, a phosphate group, a mercapto group, an isocyanate group, a nitrile group, a silicon halide group, a tin halide group and a functional group derived from an acid anhydride, in which a content of the silica (B) in the rubber composition is from 20 to 150 parts by mass on the basis of 100 parts by mass of the rubber component (A), and a content of the modified polymer (C) in the rubber composition is from 2 to 10 parts by mass on the basis of 100 parts by mass of the silica (B), and wherein the other monomer units are one or more of a conjugated diene having not more than 12 carbon atoms selected from the group consisting of butadiene, isoprene, 2,3-dimethyl-butadiene, 2-phenyl-butadiene, 1,3-pentadiene, 2-methyl-1,3-pentadiene, 1,3-hexadiene, 1,3-octadiene, 1,3-cyclohexadiene, 2-methyl-1,3-octadiene, 1,3,7-octatriene, myrcene and chloroprene. 2. The rubber composition according to claim 1 , wherein the functional group of the modified polymer (C) is at least one group selected from the group consisting of a carboxy group, an amino group, a hydroxy group and a functional group derived from an acid anhydride. 3. The rubber composition according to claim 1 , wherein the silica (B) has an average particle size of from 0.5 to 200 nm. 4. The rubber composition according to claim 1 , wherein the modified polymer (C) has a melt viscosity of from 0.1 to 3,000 Pa·s as measured at 38° C. 5. The rubber composition according to claim 1 , wherein the modified polymer (C) has a weight-average molecular weight (Mw) of from 2,000 to 500,000. 6. The rubber composition according to claim 1 , wherein the modified polymer (C) is a copolymer constituted of (c1) a monomer unit derived fromβ-farnesene and (c2) a monomer unit derived from a monomer other than β-farnesene. 7. The rubber composition according to claim 1 , further comprising a silane coupling agent in an amount of from 0.1 to 30 parts by mass on the basis of 100 parts by mass of the silica (B). 8. The rubber composition according to claim 1 , wherein the rubber component (A) comprises at least one rubber selected from the group consisting of a styrene-butadiene rubber, a butadiene rubber, an isoprene rubber and a natural rubber. 9. The rubber composition according to claim 1 , wherein the other monomer units are selected from the group consisting of butadiene, isoprene, and myrcene. 10. The rubber composition according to claim 1 , wherein the functional group is a functional group derived from an acid anhydride. 11. The rubber composition according to claim 10 , wherein the functional group derived from an acid anhydride is selected from the group consisting of a carboxylic acid anhydride group, a dicarboxylic acid group obtained by ring-opening reaction of carboxylic anhydride, a dicarboxylic acid monoester group obtained by ring-opening reaction of carboxylic anhydride and a dicarboxylic acid monoamide group obtained by ring-opening reaction of carboxylic anhydride. 12. The rubber composition according to claim 1 , wherein the rubber component (A) comprises at least one rubber selected from the group consisting of a styrene-butadiene rubber and a natural rubber. 13. The rubber composition according to claim 12 , wherein the rubber component (A) comprises the styrene-butadiene rubber, which has a weight-average molecular weight of from 100,000 to 2,500,000. 14. The rubber composition according to claim 12 , wherein the rubber component (A) comprises the styrene-butadiene rubber, which has a styrene content of from 0.1 to 70% by mass. 15. A tire comprising the rubber composition according to claim 1 in at least a part thereof.

Assignees

Inventors

Classifications

  • Silica · CPC title

  • C08L9/06Primary

    Copolymers with styrene · CPC title

  • Silicon-containing compounds {(C08K5/0091 takes precedence)} · CPC title

  • C08L7/00Primary

    Compositions of natural rubber · CPC title

  • B60C1/00Primary

    Tyres characterised by the chemical composition or the physical arrangement or mixture of the composition · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US10550248B2 cover?
The present invention provides a rubber composition capable of producing a rubber molded article that is excellent in rolling resistance performance, steering stability, mechanical strength and abrasion resistance, and a tire obtained by using the rubber composition in at least a part thereof. The present invention relates to a rubber composition including (A) a rubber component including at le…
Who is the assignee on this patent?
Kuraray Co, Amyris Inc
What technology area does this patent fall under?
Primary CPC classification C08L9/06. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue Feb 04 2020 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).