Aluminum alloy for die-casting, having improved corrosion resistance

US10525528B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-10525528-B2
Application numberUS-201715581193-A
CountryUS
Kind codeB2
Filing dateApr 28, 2017
Priority dateOct 29, 2014
Publication dateJan 7, 2020
Grant dateJan 7, 2020

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

An aluminum alloy includes 6 to 8.5 wt % of magnesium (Mg), 4 to 6 wt % of silicon (Si), 0.4 to 0.8 wt % of iron (Fe), 0.2 to 0.5 wt % of manganese (Mn), 0.01 to 0.1 wt % of copper (Cu), 0.05 to 0.15 wt % of titanium (Ti), and the remainder being aluminum (Al), and may be in use for die-casting electronic components or communication components which require weight reduction and high corrosion resistance.

First claim

Opening claim text (preview).

What is claimed is: 1. An aluminum alloy, comprising 7.82 to 7.91% by weight of magnesium (Mg), 4.5 to 4.6% by weight of silicon (Si), 0.4 to 0.8% by weight of iron (Fe), 0.2 to 0.5% by weight of manganese (Mn), 0.01 to 0.1% by weight of copper (Cu), 0.05 to 0.15% by weight of titanium (Ti), and remaining aluminum (Al). 2. The aluminum alloy according to claim 1 , further comprising at least one selected from the group consisting of beryllium (Be) and cobalt (Co) at 0.001 to 0.01% by weight. 3. The aluminum alloy according to claim 1 , wherein the aluminum alloy contains incidental impurities below 0.01% by weight.

Assignees

Inventors

Classifications

  • B22D25/02Primary

    by its peculiarity of shape; of works of art {(cylinders, pistons B22D15/02)} · CPC title

  • Dies (manufacture, see the appropriate class, e.g. B23P15/24); Die plates; Die supports; Cooling equipment for dies; Accessories for loosening and ejecting castings from dies · CPC title

  • with magnesium · CPC title

  • Forging or pressing (forging or pressing devices as units B21B15/0035) · CPC title

  • Coupling circuits between transmission lines or antennas and transmitters, receivers or amplifiers · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US10525528B2 cover?
An aluminum alloy includes 6 to 8.5 wt % of magnesium (Mg), 4 to 6 wt % of silicon (Si), 0.4 to 0.8 wt % of iron (Fe), 0.2 to 0.5 wt % of manganese (Mn), 0.01 to 0.1 wt % of copper (Cu), 0.05 to 0.15 wt % of titanium (Ti), and the remainder being aluminum (Al), and may be in use for die-casting electronic components or communication components which require weight reduction and high corrosion r…
Who is the assignee on this patent?
Kmw Inc
What technology area does this patent fall under?
Primary CPC classification B22D25/02. Mapped technology areas include Operations & Transport.
When was this patent published?
Publication date Tue Jan 07 2020 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).