Clearcoat coating composition, method for production and use
US-9617448-B2 · Apr 11, 2017 · US
US10519255B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10519255-B2 |
| Application number | US-201615759114-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jun 29, 2016 |
| Priority date | Jun 29, 2016 |
| Publication date | Dec 31, 2019 |
| Grant date | Dec 31, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Subjects of the invention are processes for preparing vinyl acetate-ethylene copolymers in the form of their aqueous dispersions or water-redispersible powders by means of radically initiated emulsion polymerization and optional subsequent drying of the resultant polymer dispersions, characterized in that the emulsion polymerization of vinyl acetate, ethylene and optionally one or more further ethylenically unsaturated monomers is carried out in the presence of one or more protective colloids in one or more Taylor reactors.
Opening claim text (preview).
The invention claimed is: 1. A process for preparing vinyl acetate-ethylene copolymers in the form of their aqueous dispersions or water-redispersible powders by means of radically initiated emulsion polymerization and optional subsequent drying of the resultant polymer dispersions, the process comprising emulsion polymerization of vinyl acetate, ethylene and optionally one or more further ethylenically unsaturated monomers in the presence of one or more protective colloids in one or more Taylor reactors, the Taylor reactor comprising an external reactor wall, a rotor located within the external reactor wall, a reactor base, and a reactor lid, the wall, rotor, base, and lid defining a toroidal reactor volume, wherein vinyl acetate, ethylene, protective colloids, and oxidation initiators are added via one or more metering devices that are embedded in the reactor base, and reduction initiators are added via one or more metering devices embedded in a bearing of the rotor. 2. The process according to claim 1 , wherein the external reactor wall has an inner wall and the rotor has an outer wall, the inner wall of the external reactor wall and the outer wall of the rotor each having a cylindrical geometry. 3. The process according to claim 1 , wherein the Taylor reactor is equipped with at least three metering devices. 4. The process according to claim 2 , wherein at least one metering device is mounted on the reactor base and/or at least one metering device ( 6 ) is mounted on a bearing of the rotor and/or at least one metering device is mounted in the external reactor wall. 5. The process according to claim 4 , wherein a plurality of metering devices ( 6 ) are mounted locally in succession in the external reactor wall in a flow direction. 6. The process according to claim 1 , wherein initiators and/or monomers comprising vinyl acetate and/or ethylene are added via one or more metering devices embedded in the external reactor wall. 7. The process according to claim 1 , having a pressure in the toroidal reactor volume of 10 to 90 bar abs. . 8. The process according to claim 1 , wherein residual monomer is removed by post-polymerization in a stirred tank or in the Taylor reactor. 9. The process according to claim 1 , wherein: vinyl acetate is polymerized with 1 to 50 wt % of ethylene; vinyl acetate is polymerized with 1 to 50 wt % of ethylene and 1 to 50 wt % of one or more vinyl esters having 3 to 12 carbon atoms in the carboxyl radical; vinyl acetate is polymerized with 1 to 50 wt % of ethylene and 1 to 60 wt % of (meth)acrylic esters of unbranched or branched alcohols having 1 to 15 carbon atoms; 30 to 75 wt % of vinyl acetate is polymerized with 1 to 30 wt % of vinyl laurate or vinyl esters of an alpha-branched carboxylic acid having 9 to 11 carbon atoms, and also 1 to 30 wt % of (meth)acrylic esters of unbranched or branched alcohols having 1 to 15 carbon atoms and 1 to 40 wt % of ethylene; or vinyl acetate is polymerized with 1 to 50 wt % of ethylene and 1 to 60 wt % of vinyl chloride; where the figures in wt % add up to 100 wt % in each case. 10. The process according to claim 1 , wherein the protective colloids comprise partially hydrolysed or fully hydrolysed polyvinyl alcohols. 11. The process according to claim 1 , wherein the polymerization is carried out in the absence of emulsifiers.
characterised by special features of the polymerisation apparatus used · CPC title
Continuous processes · CPC title
cylindrical · CPC title
resulting in a turbulent flow of the reactants, such as in centrifugal-type reactors, or having a high Reynolds-number · CPC title
Ethene · CPC title