Powder composition of polyarylene ether ketone ketones allowing an excellent castability/coalescence balance suitable for laser sintering
US-2016333190-A1 · Nov 17, 2016 · US
US10464258B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10464258-B2 |
| Application number | US-201916384055-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 15, 2019 |
| Priority date | Dec 16, 2014 |
| Publication date | Nov 5, 2019 |
| Grant date | Nov 5, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A graft copolymer comprising: a core polymer comprising a crosslinked or non-crosslinked polysaccharide, a plurality of primary graft polymers covalently grafted to the core polymer, a plurality of secondary graft polymers covalently grafted to each primary graft polymer, an injectable dermal aesthetic formulation comprising such a graft copolymer and a method of preparing such a graft copolymer.
Opening claim text (preview).
The invention claimed is: 1. A composition comprising a semicrystalline polymer having a viscosity of between 800 and 20,000 Pa·s over a time of more than 5 minutes, the viscosity measurements being carried out in a plate-plate rheometer device at a stress frequency of less than 5 rad/s, said composition being supercooled to a temperature T below the melting temperature after exposure to a temperature Tmax above its melting point, wherein the composition is configured for use in a device for manufacturing objects by melting polymer powders. 2. The composition of claim 1 , wherein the composition is a polyamide. 3. The composition of claim 1 , wherein the composition is a filled polyamide. 4. The composition of claim 1 , wherein the composition is a polyaryletherketone. 5. The composition of claim 1 , wherein the composition is a filled polyaryletherketone. 6. The composition of claim 1 , wherein the semicrystalline polymer has a viscosity of between 800 and 20,000 Pa·s over a time of more than 10 minutes. 7. The composition of claim 1 , wherein the semicrystalline polymer has a viscosity of between 1000 and 10,000 Pa·s over a time of more than 5 minutes. 8. The composition of claim 1 , wherein the semicrystalline polymer has a viscosity of between 1000 and 10,000 Pa·s over a time of more than 10 minutes. 9. The composition of claim 1 , wherein the composition is configured for use in a device for manufacturing objects by laser sintering of polymers.
Use of {PA, i.e.} polyamides, e.g. polyesteramides {or derivatives thereof,} as reinforcement · CPC title
Processes of additive manufacturing · CPC title
Use of polyethers {, e.g. PEEK, i.e. polyether-etherketone or PEK, i.e. polyetherketone or derivatives thereof,} as reinforcement · CPC title
having particular viscosity · CPC title
using layers of powder being selectively joined, e.g. by selective laser sintering or melting · CPC title