Glass-fiber-reinforced polycarbonate resin composition
US-2016024301-A1 · Jan 28, 2016 · US
US10427337B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10427337-B2 |
| Application number | US-201414902115-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 3, 2014 |
| Priority date | Jul 3, 2013 |
| Publication date | Oct 1, 2019 |
| Grant date | Oct 1, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for producing an intumescent plastic molded part that consists of a reaction plastic which contains intumescent additives and glass fibers is disclosed. The method includes providing an additive mixture which is composed of the intumescent additives and the glass fibers and mixing the additive mixture and components of the reaction plastic, where a homogeneous mass is obtained. The homogeneous mass is introduced into an injection mold and the homogeneous mass is hardened in the injection mold. A injection molding system for producing the intumescent plastic molded part and an intumescent plastic molded part are also disclosed.
Opening claim text (preview).
The invention claimed is: 1. A method for producing an intumescent plastic molded part that consists of a reaction plastic which contains intumescent additives and glass fibers, comprising the steps of: introducing the glass fibers into the intumescent additives in a mixing device and mixing the glass fibers evenly through the intumescent additives in the mixing device to form an additive mixture; introducing components of the reaction plastic by a pump into a mixing chamber through a first inlet of the mixing chamber; introducing the additive mixture from the mixing device into the mixing chamber through a second inlet of the mixing chamber; flowing a mass of the components of the reaction plastic and the additive mixture out of the mixing chamber through an outlet of the mixing chamber and into an injection mold; and hardening the mass in the injection mold. 2. The method according to claim 1 , wherein the glass fibers have a diameter of 4 μm to 10 μm and a length of 3 mm to 10 mm. 3. The method according to claim 1 , wherein a mass or a volume share of the additive mixture amounts to between 0.5% and 5% relative to the intumescent plastic molded part. 4. The method according to claim 1 , wherein the produced intumescent plastic molded part is a foamed plastic molded part. 5. The method according to claim 1 , further comprising the step of foaming the mass in the injection mold.
Flame proofing or flame retarding agents · CPC title
cellular or porous · CPC title
Mixing, kneading or conveying the foamable material (mixing plastics B29B7/00; mixing in general B01F) · CPC title
Fillers or reinforcements {, e.g. fibres} · CPC title
characterised by arrangements for controlling, measuring or regulating, e.g. for feeding or proportioning the components · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.