Surface modified carbon black to simultaneously improve rolling resistance, wet traction, and wear resistance
US-12116485-B2 · Oct 15, 2024 · US
US10407566B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10407566-B2 |
| Application number | US-201615548579-A |
| Country | US |
| Kind code | B2 |
| Filing date | Nov 25, 2016 |
| Priority date | Nov 30, 2015 |
| Publication date | Sep 10, 2019 |
| Grant date | Sep 10, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention relates to a method for preparing a low styrene-butadiene rubber having a low combined styrene content and, more particular, to a method for preparing a low styrene-butadiene rubber, wherein the low styrene-butadiene rubber contributes to an excellent polymerization rate and vulcanization rate by using an aliphatic organic acid and a sulfonate based compound as emulsifiers, and is excellent in heat stability after blending, thereby improving the workability and viscosity in in roll processing, such that the low styrene-butadiene rubber is advantageous to produce a molded article with improved rigidity and hardness when mixed with a high styrene-butadiene rubber.
Opening claim text (preview).
The invention claimed is: 1. A method for preparing styrene-butadiene rubber, comprising a step of polymerizing styrene monomer and butadiene monomer using an emulsifier, wherein the emulsifier is a mixture of an aliphatic organic acid and a sulfonate-based compound, the sulfonate-based compound includes one type selected from the group consisting of alkyl aryl sulfonates, alkali metal alkyl sulfonate, sulfonated alkyl esters and combinations thereof, the sulfonate-based compound is used in 1 part by weight to 5 parts by weight with respect to 100 parts by combined weight of the styrene monomer and the butadiene monomer, and the aliphatic organic acid and the sulfonate-based compound are used in a weight ratio of 1:1 to 10:1. 2. The method for preparing styrene-butadiene rubber of claim 1 , wherein styrene content in the styrene-butadiene rubber is of 5% by weight to 10% by weight. 3. The method for preparing styrene-butadiene rubber of claim 1 , wherein the aliphatic organic acid has a linear or branched alkyl group with 12 to 18 carbon atoms. 4. The method for preparing styrene-butadiene rubber of claim 1 , wherein the aliphatic organic acid includes one type selected from the group consisting of oleic acid, lauric acid, myristic acid, palmitic acid, stearic acid, eicosanoic acid and combinations thereof. 5. The method for preparing styrene-butadiene rubber of claim 1 , wherein the aliphatic organic acid is used in 0.5 parts by weight to 7 parts by weight with respect to 100 parts by the combined weight of the styrene monomer and the butadiene monomer.
Related publications grouped by family.
Answers are generated from the same data shown on this page.