Shrinkable face film and a label comprising a shrinkable face film
US-2017174379-A1 · Jun 22, 2017 · US
US10406786B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10406786-B2 |
| Application number | US-201314902368-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 12, 2013 |
| Priority date | Jul 12, 2013 |
| Publication date | Sep 10, 2019 |
| Grant date | Sep 10, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The invention relates to providing a method for obtaining a multilayer film for thermally inducible shrink labels, products thereof and use of such products.
Opening claim text (preview).
The invention claimed is: 1. A multilayer film for labeling comprising a first skin layer, a second skin layer and a core layer between the first skin layer and the second skin layer, wherein the core layer consists of 10 to 90% by weight of a copolymer of ethylene and butyl acrylate and 10 to 90% by weight of a copolymer of ethylene and propylene, and wherein at least one of the first skin layer and the second skin layer comprises propylene terpolymer, and wherein the multilayer film is configured to shrink in the direction of the orientation of the multilayer film in the range of 20 to 75% at a temperature range between 65 and 85° C. 2. The multilayer film according to claim 1 , wherein the copolymer of ethylene and propylene is a block or a random copolymer. 3. The multilayer film according to claim 1 , wherein the at least one of the first skin layer and the second skin layer comprises propylene terpolymer equal to or more than 95% by weight. 4. The multilayer film according to claim 1 , wherein the propylene terpolymer comprises one of: a terpolymer of ethylene, propylene and 1-butene; a terpolymer of ethylene, propylene and 1-hexene; and a terpolymer of ethylene, propylene and 1-octene. 5. The multilayer film according to claim 1 , wherein the multilayer film is configured to shrink less than 10% at a temperature below 65° C. 6. The multilayer film according to claim 1 , wherein the multilayer film is configured to shrink in the direction of the orientation of the multilayer film equal to or less than 60% at a temperature of 98° C. 7. The multilayer film according to claim 1 , wherein the multilayer film has been monoaxially stretched in the range of 4 to 7 times in a first direction wherein the first direction is parallel or perpendicular to the multilayer film machine direction. 8. The multilayer film according to claim 1 , wherein a thickness of the first skin layer is equal to a thickness of the second skin layer. 9. The multilayer film according to claim 1 , comprising an average thickness in the range of 20 to 60 micrometers after monoaxially stretched and slitted. 10. The multilayer film according to claim 1 , comprising a shrink force in the orientation direction of the multilayer film during heating at temperatures between 60 and 98° C. of less than 10N/15 mm. 11. A label comprising a length, a width and a thickness dimension, the label derived from the multilayer film according to claim 1 . 12. A method for obtaining a multilayer film for thermally inducible shrink labels, the method comprising: providing a first skin layer and a second skin layer, wherein at least one of the first skin layer and the second skin layer comprises propylene terpolymer, providing a core layer between the first skin layer and the second skin layer, wherein the core layer consists of 10 to 90% by weight of a copolymer of ethylene and butyl acrylate and 10 to 90% by weight of a copolymer of ethylene and propylene, stretching the multilayer film in the range of 4 to 7 times in a first direction for obtaining monoaxially stretched multilayer film having a tension in the first direction, and cooling the multilayer film to room temperature, wherein the multilayer film is configured to shrink in the direction of the orientation of the multilayer film in the range of 20 to 75% at a temperature range between 65 and 85° C. 13. The method according to claim 12 , further comprising providing a surface treatment for the multilayer film surface for increasing the surface tension of the first skin layer or the second skin layer. 14. The method according to claim 12 , wherein the first skin layer and the second skin layer have been provided by extrusion or casting. 15. The method according to claim 12 , wherein the first direction is parallel or perpendicular to the multilayer film machine direction.
Packaging equipment or accessories not otherwise provided for · CPC title
comprising acrylic (co)polymers · CPC title
by clamping action (by separate clamps G09F3/16) · CPC title
using fillers, pigments, thixotroping agents · CPC title
Labels, badges · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.