Gel pulverization device, method for manufacturing polyacrylic acid (polyacrylate) superabsorbent polymer powder, and superabsorbent polymer powder
US-9533433-B2 · Jan 3, 2017 · US
US10406256B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10406256-B2 |
| Application number | US-201414914150-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 28, 2014 |
| Priority date | Aug 28, 2013 |
| Publication date | Sep 10, 2019 |
| Grant date | Sep 10, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a water absorbent resin that is useful to sanitary materials such as a disposable diaper, a sanitary napkin, and a blood absorbent for medical use each having a higher liquid permeability and a higher water absorbing speed. Further provided is a water absorbent resin powder that is useful to sanitary materials such as a disposable diaper, a sanitary napkin, and a blood absorbent for medical use each having increased in absorbency of a liquid and in heat retaining property. A gel grinding device to be used to produce a water absorbent resin, includes: a screw; a feed opening; an extrusion opening; a porous plate; and a barrel, the barrel including a return preventing member provided on an inner surface thereof, and the return preventing member satisfying at least one of specific parameters.
Opening claim text (preview).
The invention claimed is: 1. A method for producing a polyacrylic acid (salt)-based water absorbent resin powder, comprising: a polymerization step of polymerizing an acrylic acid (salt)-based monomer aqueous solution to form a polyacrylic acid (salt)-based hydrogel-like crosslinked polymer having a resin solid content of 10 wt % to 80 wt %; a gel grinding step, carried out during or after the polymerization, of carrying out gel grinding with respect to the hydrogel-like crosslinked polymer to form a particulate polyacrylic acid (salt)-based hydrogel-like crosslinked polymer; and a drying step carried out after the gel grinding, in the gel grinding step, the hydrogel-like crosslinked polymer being ground by use of a gel grinding device comprising: a screw; a feed opening; an extrusion opening; a porous plate; and a barrel, the barrel including at least one return preventing member provided on an inner surface of the barrel, and the barrel satisfying at least one of the following (1) and (2): (1) 0.05≤YH/N≤0.25; and (2) 0.05≤YF/N≤0.25 where YH is a height of the at least one return preventing member which height is obtained by cutting the barrel in a direction vertical to a direction in which a gel of the water absorbent resin is extruded; YF is a width of a top surface of the at least one return preventing member, the width being along a direction vertical to a direction in which the at least one return preventing member extends; and N is a diameter of an inner part of the barrel which diameter does not include the at least one return preventing member. 2. The method as set forth in claim 1 , wherein T/N 3 ranges from 0.05 to 2.0 where T is an amount [g/hr] in which the gel grinding device treats a hydrogel per hour and T/N 3 is a treatment amount-to-inner diameter ratio [g/hr/mm 3 ] that is a treatment amount per unit time of the gel grinding device. 3. The method as set forth in claim 1 , wherein the particulate polyacrylic acid (salt)-based hydrogel-like crosslinked polymer which is obtained in the gel grinding step is dried under a condition where a through-flow belt-type dryer is used, a drying temperature is 150° C. to 250° C., and hot air blows in a vertical direction (an up-and-down direction) at an air velocity of 0.8 [m/s] to 2.5 [m/s]. 4. The method as set forth in claim 1 , wherein the barrel of the gel grinding device has a temperature of 40° C. to 120° C. while the gel grinding step is being carried out.
Screws (B29B7/421 takes precedence) · CPC title
Parts or accessories, e.g. casings, feeding or discharging means · CPC title
with screw sections co-operating, e.g. intermeshing, with elements on the wall of the surrounding casing · CPC title
Powdering or granulating · CPC title
having projections with a short length in the barrel direction, e.g. pins · CPC title