Polymer compound, intermediate composition, negative electrode, electricity storage device, slurry for negative electrodes, method for producing polymer compound, and method for producing negative electrode
US-2017331114-A1 · Nov 16, 2017 · US
US10351672B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10351672-B2 |
| Application number | US-201716075753-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jan 30, 2017 |
| Priority date | Feb 18, 2016 |
| Publication date | Jul 16, 2019 |
| Grant date | Jul 16, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A polymer compound is formed by condensing a polyacrylic acid, a polyfunctional amine represented by the following general formula (1), and an aromatic monoamine. A chain structure constituted by the polyacrylic acid has free carboxyl groups and carboxyl groups to which the aromatic monoamines are bonded. Y is a straight-chain alkyl group having 1 to 4 carbon atoms, a phenylene group, or an oxygen atom. R1 and R2 are each independently one or more hydrogen atoms, a methyl group, an ethyl group, a trifluoromethyl group, or a methoxy group.
Opening claim text (preview).
The invention claimed is: 1. A polymer compound to be used as a binder for a negative electrode of a power storage device, wherein the polymer compound is formed by condensing a polyacrylic acid, a polyfunctional amine represented by the following general formula (1), and an aromatic monoamine, a chain structure constituted by the polyacrylic acid has free carboxyl groups and carboxyl groups to which the aromatic monoamines are bonded: where Y is a straight-chain alkyl group having 1 to 4 carbon atoms, a phenylene group, or an oxygen atom, and R1 and R2 are each independently one or more hydrogen atoms, a methyl group, an ethyl group, a trifluoromethyl group, or a methoxy group. 2. A negative electrode of a power storage device, comprising: a binder for a negative electrode containing a polymer compound according to claim 1 , and a negative electrode active substance, wherein the negative electrode active substance is at least one selected from carbon-based materials capable of occluding and releasing lithium, elements alloyable with lithium, and compounds having an element alloyable with lithium. 3. The negative electrode according to claim 2 , wherein the negative electrode active substance is at least one selected from silicon materials obtained from CaSi 2 through a calcium-removal reaction, Si and SiO v , in which 0<V≤2. 4. A power storage device comprising: the negative electrode according to claim 3 ; and a nonaqueous electrolyte. 5. An intermediate composition of a polymer compound to be used as a binder for a negative electrode of a power storage device, the intermediate composition being in a liquid state and containing a polyacrylic acid, a polyfunctional amine represented by the following general formula (1), an aromatic monoamine, and a nonaqueous solvent: where Y is a straight-chain alkyl group having 1 to 4 carbon atoms, a phenylene group or an oxygen atom, and R1 and R2 are each independently one or more hydrogen atoms, a methyl group, an ethyl group, a trifluoromethyl group, or a methoxy group. 6. A slurry for a negative electrode to be used for production of a negative electrode of a power storage device, wherein the slurry contains the intermediate composition according to claim 5 , a negative electrode active substance, and a solvent, and the negative electrode active substance is at least one selected from carbon-based materials capable of occluding and releasing lithium, elements alloyable with lithium, and compounds having an element alloyable with lithium. 7. A method for producing a negative electrode of a power storage device, wherein a negative electrode active substance layer is formed on a current collector by using a slurry for the negative electrode according to claim 6 . 8. The method for producing a negative electrode according to claim 7 , wherein the slurry for a negative electrode contains, as the negative electrode active substance, at least one selected from silicon materials obtained from CaSi2 through a calcium-removal reaction, Si, and SiO v in which 0<V≤2. 9. A polymer compound to be used as a binder for a negative electrode of a power storage device, wherein the polymer compound has a chain structure constituted by a polyacrylic acid, and a crosslinked structure connecting carboxyl groups in the chain structure or between the chain structures with each other, the crosslinked structure is at least one crosslinked structure selected from the following general formulae (2) to (4), and the chain structure has free carboxyl groups and carboxyl groups to which aromatic monoamines are bonded: where PAA denotes the chain structure constituted by the polyacrylic acid; and X is a structure represented by the following general formula (5): where Y is a straight-chain alkyl group having 1 to 4 carbon atoms, a phenylene group, or an oxygen atom, and R1 and R2 are each independently a hydrogen atom, a methyl group, a trifluoromethyl group, or a methoxy group. 10. The polymer compound according to claim 9 , wherein a proportion of the carboxyl group to which the aromatic monoamine is bonded to the free carboxyl group is in the range of 0.001 to 0.15. 11. A method for producing a polymer compound according to claim 9 , comprising heating a polyacrylic acid, a polyfunctional amine represented by the following general formula (1), and an aromatic monoamine at 150 to 230° C.: where Y is a straight-chain alkyl group having 1 to 4 carbon atoms, a phenylene group, or an oxygen atom, and R1 and R2 are each independently one or more hydrogen atoms, a methyl group, an ethyl group, a trifluoromethyl group, or a methoxy group. 12. A negative electrode of a power storage device, comprising: a binder for a negative electrode containing a polymer compound according to claim 9 ; and a negative electrode active substance, wherein the negative electrode active substance is at least one selected from carbon-based materials capable of occluding and releasing lithium, elements alloyable with lithium, and compounds having an element alloyable with lithium.
using polymerised unsaturated fatty acids · CPC title
Polyamide-imides · CPC title
Electrodes based on metals, Si or alloys · CPC title
Selection of inactive substances as ingredients for active masses, e.g. binders, fillers · CPC title