Methods of making and using cement coated substrate
US-9896903-B2 · Feb 20, 2018 · US
US10323171B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10323171-B2 |
| Application number | US-201916259579-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jan 28, 2019 |
| Priority date | Jul 20, 2017 |
| Publication date | Jun 18, 2019 |
| Grant date | Jun 18, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Portland cement clinker LCMs that include Portland cement clinker to mitigate or prevent lost circulation in a well are provided. A Portland cement clinker LCM may include Portland cement clinker, Portland cement, a carrier fluid, and an inorganic consolidation activator. Another Portland cement clinker LCM may include Portland cement clinker and a crosslinked fluid, such as a polyuronide crosslinked via calcium ions or a polysaccharide crosslinked via divinyl sulfone. Yet another Portland cement clinker LCM may include Portland cement clinker and polymer fibers or particulate glass. Methods of lost circulation control using a Portland cement clinker LCM are also provided.
Opening claim text (preview).
What is claimed is: 1. A lost circulation material (LCM) composition, comprising: Portland cement clinker, wherein the Portland cement clinker consists of non-hydraulic, non-cementiceous unground Portland cement clinker particles; cement; a carrier fluid; a plurality of polymer fibers; and an inorganic consolidation activator selected to consolidate the clinker in the composition to form a plug when introduced into a lost circulation zone. 2. The LCM composition of claim 1 , wherein the Portland cement clinker comprises ASTM International Type I cement clinker, ASTM International Type V cement clinker, API Class A cement clinker, or API Class G cement clinker. 3. The LCM composition of claim 1 , wherein the cement comprises API Class G cement. 4. The LCM composition of claim 1 , wherein the inorganic consolidation activator comprises a silicate salt. 5. The LCM composition of claim 1 , wherein the inorganic consolidation activator comprises at least one of sodium silicate, calcium aluminate, calcium chloride, sodium aluminate, and potassium silicate. 6. The LCM composition of claim 1 , wherein the inorganic consolidation activator comprises an amount in the range of about 1.0 weight of the total weight (w/w %) to about 3.0 w/w %. 7. The LCM composition of claim 1 , wherein the weight ratio of carrier fluid to clinker is 1:1. 8. The LCM composition of claim 1 , wherein the weight ratio of cement clinker to cement is in the range of 60:40 to 70:30. 9. The LCM composition of claim 1 , wherein the polymer fibers comprise polypropylene fibers.
Cross-linked polymers · CPC title
containing organic compounds · CPC title
Aluminates · CPC title
according to API · CPC title
Plastering the borehole wall; Injecting into the formation · CPC title
Related publications grouped by family.