Active material excelling in high-voltage characteristics
US-2015357641-A1 · Dec 10, 2015 · US
US10312513B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10312513-B2 |
| Application number | US-201515309859-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 7, 2015 |
| Priority date | May 13, 2014 |
| Publication date | Jun 4, 2019 |
| Grant date | Jun 4, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A lithium composite metallic oxide expressed by: LiaNibCocMndDeOf (where 0.2≤“a”≤1.5, “b”+“c”+“d”+“e”=1, 0<“e”<1, “D” is at least one of the following elements: Fe, Cr, Cu, Zn, Ca, Mg, Zr, S, Si, Na, K, Al, Ti, P, Ga, Ge, V, Mo, Nb, W, La, Hf and Rf, and 1.7≤“f”≤2.1), and including: a high manganese portion, which is made of a metallic oxide including Ni, Co and Mn at least and of which the composition ratio between Ni, Co and Mn is expressed by Ni:Co:Mn=g:h:i (note that “g”+“h”+“i”=1, 0<“g”<1, 0<“h”<“c”, and “d”<“i”<1), in a superficial layer thereof; and a metallic oxidation portion in an outermost superficial layer of the high manganese portion.
Opening claim text (preview).
The invention claimed is: 1. A lithium composite metallic oxide expressed by a general formula, Li a Ni b Co c Mn d D e O f where 0.2≤“a”≤1.5, “b”+“c”+“d”+“e”=1, 0<“e”<1,“D” is at least one element selected from the group consisting of Fe, Cr, Cu, Zn, Ca, Mg, Zr, S, Si, Na, K, Al, Ti, P, Ga, Ge, V, Mo, Nb, W, La, Hf, and Rf, and 1.7≤“f”≤2.1; the lithium composite metallic oxide comprising: a high manganese portion, which is made of a metallic oxide including Ni, Co and Mn at least and of which the composition ratio between Ni, Co and Mn is expressed by Ni:Co:Mn=g:h:i where “g”+“h”+“i”=1, 0<“g”<1, 0<“h”<“c”, and “d”<“i”<1, in a superficial layer thereof; and a metallic oxidation portion in an outermost superficial layer of the high manganese portion, the metallic oxidation portion is expressed by a formula Li q M 2 O 3+r , where 0<“q”<1, 0≤“r”<1, M is a metal selected from the group consisting of Ni, Co and Mn, and the composition of the metallic oxidation portion is different from the composition of the high manganese portion; the lithium composite metallic oxide further comprising: a first-composition portion expressed by a general formula, Li a1 Ni b1 Co c1 Mn d1 D e1 O f1 where 0.2≤“a 1 ”≤1.5, “b 1 ”+“c 1 ”+“d 1 ”+“e 1 ”=1, 0<“e 1 ”<1, “D” is at least one element selected from the group consisting of Fe, Cr, Cu, Zn, Ca, Mg, Zr, S, Si, Na, K, Al, Ti, P, Ga, Ge, V, Mo, Nb, W, La, Hf and Rf, and 1.7≤“f 1 ”≤2.1; and a second-composition portion expressed by a general formula, Li a2 Ni b2 Co c2 Mn d2 D e2 O f2 where 0.2≤“a 2 ”≤1.5, “b 2 ”+“c 2 ”+“d 2 ”+“e 2 ”=1, 0<“e 2 ”<1, “D” is at least one element selected from the group consisting of Fe, Cr, Cu, Zn, Ca, Mg, Zr, S, Si, Na, K, Al, Ti, P, Ga, Ge, V, Mo, Nb, W, La, Hf and Rf, and 1.7≤“f 2 ”≤2.1 where at least any of the following is satisfied: “c 2 ”<“c 1 ”; or “d 2 ”>“d 1 ”. 2. The lithium composite metallic oxide as set forth in claim 1 , wherein the metallic oxidation portion includes a crystal. 3. The lithium composite metallic oxide as set forth in claim 1 , wherein the second-composition portion satisfies both of the following: “d 2 ”>“d 1 ”; and “e 2 ”<“e 1 ”. 4. A production process for the lithium composite metallic oxide as set forth in claim 1 , the production process comprising any of following Treatments 1 through 5 carried out to a material expressed by a general formula, Li a Ni b Co c Mn d D e O f (where 0.2≤“a”≤1.5, “b”+“c”+“d”+“e”=1, 0<“e”<1, “D” is at least one element selected from the group consisting of Fe, Cr, Cu, Zn, Ca, Mg, Zr, S, Si, Na, K, Al, Ti, P, Ga, Ge, V, Mo, Nb, W, La, Hf and Rf, and 1.7≤“f”≤2.1): (Treatment 1) comprising the steps of: 1-1) readying an acidic metallic salt aqueous solution; 1-2) mixing the acidic metallic salt aqueous solution with the aforementioned material; 1-3) mixing a liquid obtained at said step 1-2) with an ammonium-phosphate salt aqueous solution; and 1-4) isolating the lithium composite metallic oxide from another liquid obtained at said step 1-3); (Treatment 2) comprising the steps of: 2-1) readying an ammonium-phosphate salt aqueous solution; 2-2) mixing the ammonium-phosphate salt aqueous solution with the aforementioned material; 2-3) mixing a liquid obtained at said step 2-2) with an acidic metallic salt aqueous solution; and 2-4) isolating the lithium composite metallic oxide from another liquid obtained at said step 2-3); (Treatment 3) comprising the steps of: 3-1) readying an aqueous solution of an ammonium-phosphate salt, or an aqueous solution of a metallic salt and an ammonium-phosphate salt; 3-2) mixing the aqueous solution with the aforementioned material; and 3-3) isolating the lithium composite metallic oxide from a liquid obtained at said step 3-2); (Treatment 4) comprising the steps of: 4-1) readying an acidic metallic salt aqueous solution, and an ammonium-phosphate salt aqueous solution, respectively; 4-2) mixing water with the aforementioned material; 4-3) mixing a liquid obtained at said step 4-2), said acidic metallic salt aqueous solution, and said ammonium-phosphate salt aqueous solution each other; and 4-4) isolating the lithium composite metallic oxide from another liquid obtained at said step 4-3); or (Treatment 5) comprising the steps of: 5-1) readying a metallic phosphate salt aqueous solution, or a metallic polyphosphate salt aqueous solution; 5-2) mixing the aqueous solution with the aforementioned material; and 5-3) isolating the lithium composite metallic oxide from a liquid obtained at said step 5-2). 5. A lithium-ion secondary battery comprising the lithium composite metallic oxide as set forth in claim 1 .
Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries · CPC title
obtained by TEM, STEM, STM or AFM · CPC title
by XPS, EDX or EDAX data · CPC title
Cross-Sectional Technologies · mapped topic
of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy · CPC title