Resin composition for blow hollow molded articles, blow hollow molded article and method for producing same
US-2016319109-A1 · Nov 3, 2016 · US
US10280304B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10280304-B2 |
| Application number | US-201515039485-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jan 28, 2015 |
| Priority date | Feb 5, 2014 |
| Publication date | May 7, 2019 |
| Grant date | May 7, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The resin composition comprises (A) 100 parts by weight of a polyarylene sulfide resin (component A) synthesized through a polymerization reaction using an aromatic disulfide-based compound as a polymerization terminator and (B) 10 to 180 parts by weight of carbon fibers (component B), wholly aromatic polyamide fibers (component C) or glass fibers (component D).
Opening claim text (preview).
The invention claimed is: 1. A resin composition produced by melt kneading components comprising: (A) 100 parts by weight of a polyarylene sulfide resin (component A) synthesized through a polymerization reaction using an aromatic disulfide-based compound as a polymerization terminator, and (C) 10 to 150 parts by weight of a fiber (component C), wherein the component C is at least one selected from the group consisting of a para-aramid fiber and a meta-aramid fiber, based on 100 parts by weight of the component A, wherein the component C has a fiber length of 0.1 to 3 mm, and wherein the component C is sized with at least one sizing agent selected from the group consisting of a polyester, a polyurethane and a polyether sulfone resin. 2. The resin composition according to claim 1 , wherein the aromatic disulfide-based compound is at least one selected from the group consisting of a benzothiazole and a diphenyl disulfide. 3. A molded article comprising the resin composition of claim 2 . 4. The resin composition according to claim 1 , wherein the aromatic disulfide-based compound is at least one selected from the group consisting of diphenyl disulfide and dithiobisbenzothiazole. 5. A molded article comprising the resin composition of claim 4 . 6. The resin composition according to claim 1 , wherein the component A is a polyarylene sulfide resin obtained by directly heating and polymerizing a diiodoaryl compound, solid sulfur and an aromatic disulfide-based compound without using a polar solvent. 7. A molded article comprising the resin composition of claim 6 . 8. A molded article comprising the resin composition of claim 1 . 9. The resin composition according to claim 1 , wherein the composition has a dynamic friction coefficient of not more than 0.47. 10. The resin composition according to claim 1 , wherein the composition has an impact strength of 12 KJ/m 2 or more.
Polyamides derived from aromatically bound amino and carboxyl groups of amino-carboxylic acids or of polyamines and polycarboxylic acids · CPC title
Glass · CPC title
Ingredients treated with inorganic substances · CPC title
Polythioethers; Polythioether-ethers · CPC title
Carbon · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.