Process of preparing a chemically pre-formed (cpf) iron negative electrode with oxidizing compounds
US-2015060740-A1 · Mar 5, 2015 · US
US10217994B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10217994-B2 |
| Application number | US-201815938594-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 28, 2018 |
| Priority date | Sep 5, 2013 |
| Publication date | Feb 26, 2019 |
| Grant date | Feb 26, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a Ni—Fe battery comprising an iron electrode which is preconditioned prior to any charge-discharge cycle. The preconditioned iron electrode used in the Ni—Fe battery is prepared by first fabricating an electrode comprising an iron active material, and then treating the surface of the electrode with an oxidant to thereby create an oxidized surface.
Opening claim text (preview).
What is claimed is: 1. A Ni—Fe battery comprising an electrode comprising an iron active material, which electrode has been preconditioned prior to any charge-discharge cycle to have the accessible surface of the iron material in the same oxidation state as discharged iron negative electrode active material. 2. The battery of claim 1 , wherein the oxidation state of the conditioned iron active material is +2, +2/+3, +3 or +4. 3. The battery of claim 1 , wherein the electrode further comprises a binder. 4. The battery of claim 1 , wherein the electrode further comprises sulfur. 5. The battery of claim 1 , wherein the electrode further comprises a conductive additive. 6. The battery of claim 5 , wherein the conductive additive comprises nickel, or copper or carbon black. 7. The battery of claim 1 , wherein the electrode comprises an iron active material comprising about: 50-90 wt % iron powder 5-30 wt % nickel powder 0.5-5.0 w % binder, and 0.25-20 w % sulfur. 8. The battery of claim 1 , wherein the electrode comprise a single layer of conductive substrate coated on at least one side with a coating comprising the iron active material. 9. The battery of claim 8 , wherein the substrate of the electrode is comprised of nickel plated steel. 10. The battery of claim 1 , wherein the porosity of the electrode is in the range of about 15-50%. 11. A battery of claim 1 , wherein the iron electrode is prepared by a process comprising: i) fabricating an electrode comprising an iron active material, and ii) treating the surface of the electrode with an oxidant to thereby create an oxidized surface. 12. The battery of claim 11 , therein the oxidant comprises water, hydrogen peroxide, ozone, chlorine, nitric acid, hypochlorite, nitrous oxide, bromine, iodine, permanganate compounds, or sodium perborate. 13. The battery of claim 11 , wherein the oxidant comprises water or hydrogen peroxide. 14. The battery of claim 11 , wherein the oxidant comprises a gaseous oxidant.
Processes of manufacture · CPC title
Selection of inactive substances as ingredients for active masses, e.g. binders, fillers · CPC title
Electric conductive fillers · CPC title
Manufacturing of an active layer by chemical means · CPC title
Iron electrodes · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.