Method For Producing An Electrode For A Lithium Accumulator And Associated Electrode
US-2015303462-A1 · Oct 22, 2015 · US
US10214454B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10214454-B2 |
| Application number | US-201816040785-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 20, 2018 |
| Priority date | Nov 15, 2016 |
| Publication date | Feb 26, 2019 |
| Grant date | Feb 26, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for manufacturing micropowder is provided, which includes (a) mixing a silicon precursor and a carbon precursor to form a mixture, and heating and keeping the mixture at 1600° C. to 1800° C. under a vacuum and non-oxygen condition for 120 to 180 minutes to form a silicon carbide powder; and (b) heating and keeping the silicon carbide powder at 1900° C. to 2100° C. under non-oxygen condition for 5 to 15 minutes, and then cooling and keeping the silicon carbide powder at 1800° C. to 2000° C. under the non-oxygen condition for 5 to 15 minutes to form micropowder, wherein the micropowder includes a silicon carbide core covered by a carbon film.
Opening claim text (preview).
What is claimed is: 1. Micropowder, comprising: a silicon carbide core; and a carbon film covering the silicon carbide core, wherein the silicon carbide core has a diameter of 50 micrometers to 500 micrometers, and the carbon film has a thickness of 20 nm to 200 nm, wherein the micropowder is a hexagonal structure. 2. The micropowder as claimed in claim 1 , having an emission wavelength of 400 nm to 550 nm.
Apparatus for preparing, pre-treating the source material to be used for crystal growth · CPC title
Single-crystal growth by condensing evaporated or sublimed materials · CPC title
Alkoxides, e.g. methoxide, tert-butoxide · CPC title
characterised by the applied pressure or type of atmosphere, e.g. in vacuum, hydrogen or a specific oxygen pressure · CPC title