Aluminum alloy flux-cored welding wire and fabrication method thereof
US-2024227087-A1 · Jul 11, 2024 · US
US10207372B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10207372-B2 |
| Application number | US-201414913637-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 15, 2014 |
| Priority date | Aug 23, 2013 |
| Publication date | Feb 19, 2019 |
| Grant date | Feb 19, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
An aluminum composite material includes a first metallic plate, a second metallic plate, and a matrix material that is interposed between the first metallic plate and the second metallic plate and is formed of aluminum powder. Gadolinium oxide particles are dispersed in the matrix material.
Opening claim text (preview).
The invention claimed is: 1. An aluminum composite material comprising: a first metallic plate; a second metallic plate; and a matrix material that is interposed between the first metallic plate and the second metallic plate and is formed of aluminum powder, wherein the matrix material contains gadolinium oxide particles in an amount of 6% by mass or more and 15% by mass or less, and the aluminum composite material has a percentage elongation of 12.6% or more and 20.8% or less. 2. An aluminum composite material comprising: a first metallic plate; a second metallic plate; and a matrix material that is interposed between the first metallic plate and the second metallic plate and is formed of aluminum powder, wherein the matrix material contains gadolinium oxide particles in an amount of 2% by mass or more and 20% by mass or less and contains boron carbide particles in an amount of 10% by mass or more and 20% by mass or less, and the aluminum composite material has a 0.2% yield strength of 127 MPa or more and 139 MPa or less. 3. An aluminum composite material comprising: a first metallic plate; a second metallic plate; and a matrix material that is interposed between the first metallic plate and the second metallic plate and is formed of aluminum powder, wherein the matrix material contains gadolinium oxide particles in an amount of 2% by mass or more and 10% by mass or less and contains boron carbide particles in an amount of 10% by mass or more and 20% by mass or less, and the aluminum composite material has a percentage elongation of 6.7% or more and 11.2% or less.
Matrix based on Al, Mg, Be or alloys thereof · CPC title
Non-ferrous alloys containing at least 5% by weight but less than 50% by weight of oxides, carbides, borides, nitrides, silicides or other metal compounds, e.g. oxynitrides, sulfides, whether added as such or formed in situ · CPC title
Powders, particles or spheres; Preforms made therefrom · CPC title
Processes characterised by the sequence of their steps · CPC title
Operations & Transport · mapped topic
Related publications grouped by family.
Answers are generated from the same data shown on this page.