Core positioning
US-2015377038-A1 · Dec 31, 2015 · US
US10166598B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10166598-B2 |
| Application number | US-201414893101-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 28, 2014 |
| Priority date | May 29, 2013 |
| Publication date | Jan 1, 2019 |
| Grant date | Jan 1, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A coating layer including solely silicon alkoxide or mixed alkoxide of silicon alkoxide and aluminum alkoxide is formed on a surface of a sintered precision-casting core body mainly including silica particles so as to seal holes formed in the surface. As a result, it is possible to prevent the breakage of the core during casting.
Opening claim text (preview).
The invention claimed is: 1. A precision-casting core obtained by forming a coating layer of two kinds of silica materials having different particle diameters on a surface of a sintered precision-casting core body mainly including silica particles, wherein the two kinds of silica materials having different particle diameters comprise silica sol and silica fume having larger particle diameters than the silica sol, the silica fume consisting of spherical particles, and the silica sol and the silica fume have a weight ratio of 1:1 to 2:1. 2. A precision-casting mold used to manufacture cast metal, comprising: a precision-casting core obtained by forming a coating layer of two kinds of silica materials having different particle diameters on a surface of a sintered precision-casting core body mainly including silica particles having a shape corresponding to a cavity inside the cast metal; and an outer mold corresponding to the shape of the outer peripheral surface of the cast metal, wherein the two kinds of silica materials having different particle diameters comprise silica sol and silica fume having larger particle diameters than the silica sol, the silica fume consisting of spherical particles, and the silica sol and the silica fume have a weight ratio of 1:1 to 2:1. 3. A precision-casting core manufacturing method comprising: immersing a sintered body of a precision-casting core body mainly including silica particles into a coating material including two kinds of silica materials having different particle diameters; drying the sintered body; and heating the sintered body so as to form a coating layer on the surface of the precision-casting core body, wherein the two kinds of silica materials having different particle diameters comprise silica sol and silica fume having larger particle diameters than the silica sol, the silica fume consisting of spherical particles, and the silica sol and the silica fume have a weight ratio of 1:1 to 2:1.
Use of lost patterns · CPC title
Cores; Manufacture or installation of cores {(breaker cores B22C9/084)} · CPC title
Sand moulds or like moulds for shaped castings · CPC title
for hollow articles · CPC title
Selection of compositions for coating the surfaces of moulds, cores, or patterns · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.