Nonaqueous secondary battery and method for manufacturing same

US10141547B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-10141547-B2
Application numberUS-201414899866-A
CountryUS
Kind codeB2
Filing dateJun 19, 2014
Priority dateJun 21, 2013
Publication dateNov 27, 2018
Grant dateNov 27, 2018

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A nonaqueous secondary battery which can be made thinner without deterioration of battery performance, and a method for manufacturing the battery. The nonaqueous secondary battery includes a positive electrode and a negative electrode which are substantially arranged in the same plane so that respective end surfaces face each other at a distance; a substrate by which the positive electrode and the negative electrode are affixed and supported; a cover member having gas barrier properties, which defines an airtight chamber together with the substrate, in the chamber in which the positive electrode and the negative electrode are contained; and an electrolyte which is contained in the airtight chamber so as to be positioned at least between the facing end surfaces of the positive electrode and the negative electrode, and which relates to the battery reaction between the positive electrode and the negative electrode.

First claim

Opening claim text (preview).

The invention claimed is: 1. A nonaqueous secondary battery comprising: a positive electrode; a negative electrode; a substrate; a cover member; and an electrolyte, wherein the positive electrode and the negative electrode are arranged in substantially the same plane and respective end surfaces of the positive electrode and the negative electrode face each other at a distance; the substrate fixingly supports the positive electrode and the negative electrode; the cover member has gas barrier properties and defines an airtight chamber together with the substrate; the cover member comprises glass, a glass film, or silicon, and a noble metal or a hydrofluoric acid-resistant inorganic oxide selected from the group consisting of Al 2 O 3 , ZrO 2 , ZnO, Nb 2 O 5 , Ta 2 O 5 , and TiO 2 is vapor-deposited to the cover member which is brought into contact with the electrolyte; the airtight chamber contains the positive electrode and the negative electrode; the electrolyte is contained in the airtight chamber and is configured to be present at least between the facing end surfaces of the positive electrode and the negative electrode. 2. The battery according to claim 1 , wherein the cover member has hydrofluoric acid-resistance. 3. A method for manufacturing the nonaqueous secondary battery according to claim 1 , the method comprising: forming a positive electrode and a negative electrode both on a substrate, respective end surfaces of the positive electrode and the negative electrode facing each other at a distance; bonding a cover member to the substrate, the cover member being configured to define an airtight chamber together with the substrate, the airtight chamber containing the positive electrode and the negative electrode; and filling the airtight chamber with an electrolyte which is present at least between the facing end surfaces of the positive electrode and the negative electrode. 4. A method for manufacturing the nonaqueous secondary battery according to claim 1 , the method comprising: forming a positive electrode and a negative electrode both on a substrate, respective end surfaces of the positive electrode and the negative electrode facing each other at a distance; disposing an electrolyte at least between facing end surfaces of the positive electrode and the negative electrode; providing a cover member by any one of methods (1) to (4) below; and fixing the cover member to the substrate, the cover member being configured to define an airtight chamber together with the substrate, the airtight chamber containing the positive electrode and the negative electrode, and the airtight is being filled with the electrolyte, wherein the electrolyte is a gel electrolyte or a solid electrolyte, wherein the methods are: (1) attaching a coating film to the electrolyte directly or through an adhesive agent; (2) forming a coating membrane made of gas barrier material by film-forming organic or inorganic gas barrier material on the electrolyte or on the coating film attached to the electrolyte by an application process or a vacuum film-formation process; and (3) forming a film of metal on the electrolyte or the coating film attached to the electrolyte or a coating membrane made of the organic gas barrier material by a coating process or a vacuum film formation process, or the like, (4) forming a coating membrane made of inorganic compound coating material on the electrolyte or the coating film attached to the electrolyte or a coating membrane made of the organic gas barrier material by a coating process or a vacuum film formation process, or the like. 5. The method according to claim 3 , wherein the forming comprises: forming a current collector by forming a conductive layer on a surface of the substrate, and patterning the conductive layer, applying a resist composition and forming a resist layer on a surface of the substrate including the current collector, forming a guide hole configured to form a positive electrode or a negative electrode above the current collector by irradiating the surface of the resist layer with light through a mask and developing the resist layer, and forming an active material layer on a surface of the current collector by using the guide hole as a casting mold. 6. The method according to claim 4 , wherein the forming comprises: forming a current collector by forming a conductive layer on a surface of the substrate, and patterning the conductive layer; applying a resist composition and forming a resist layer on a surface of the substrate including the current collector; forming a guide hole configured to form a positive electrode or a negative electrode above the current collector by irradiating the surface of the resist layer with light through a mask and developing the resist layer; and forming an active material layer on a surface of the current collector using the guide hole as a casting mold. 7. The method according to claim 3 , wherein filling of the electrolyte is carried out by immersing the airtight chamber comprising the cover member and the substrate into the electrolyte and reducing pressure or infusion using a syringe. 8. The method according to claim 3 , wherein filling of the electrolyte is carried out through a liquid injection hole formed on a lateral surface of the cover member. 9. The method according to claim 3 , wherein the cover member is produced by laminating blasting resist on glass, carrying out exposure and development to expose a blast-processed surface, carrying out sandblast processing to dig down the blast-processed surface, and stripping off the resist. 10. The method according to claim 3 , wherein both the positive electrode and the negative electrode are comb-shaped, and in a region in which the teeth of both comb-shaped electrodes are alternately arranged in the direction perpendicular to the direction of the length of teeth in the both comb-shaped electrodes and in the direction parallel to the substrate, an area ratio of a transmission portion to the total area of the teeth of the both comb-shaped electrodes, and a gap (transmission portion) between the teeth of the comb-shaped electrode being the positive electrode and the teeth of the comb-shaped electrode being the negative electrode is 40 to 95%. 11. The method according to claim 4 , wherein both the positive electrode and the negative electrode are comb-shaped, and in a region in which the teeth of the both comb-shaped electrodes are alternately arranged seen in the direction perpendicular to the direction of the length of teeth in the both comb-shaped electrodes and in the direction parallel to the substrate, an area ratio of a transmission portion to the total area of the teeth of the both comb-shaped electrodes, and a gap (transmission portion) between the teeth of the comb-shaped electrode being the positive electrode and the teeth of the comb-shaped electrode being the negative electrode is 40 to 95%. 12. The method according to claim 3 , wherein the forming comprises: (a) forming a current collector by forming a conductive layer on a surface of the substrate, and patterning the conductive layer; (b) applying a resist composition and forming a resist layer on a surface of the substrate including the current collector; (c) forming a guide hole configured to form a positive electrode or a negative electrode above the current collector by irradiating the surface of the resist layer with light through a mask and developing the resist layer; (d) forming an active material layer on a surface of the current collector by using the guide hole as a casting mold; and The (b) applying, (c) forming, and (d) forming is performed b

Assignees

Inventors

Classifications

  • H01M10/058Primary

    Construction or manufacture · CPC title

  • Thickness · CPC title

  • for protecting against corrosion · CPC title

  • prismatic or rectangular (H01M50/109, H01M50/11 take precedence) · CPC title

  • Metals · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US10141547B2 cover?
A nonaqueous secondary battery which can be made thinner without deterioration of battery performance, and a method for manufacturing the battery. The nonaqueous secondary battery includes a positive electrode and a negative electrode which are substantially arranged in the same plane so that respective end surfaces face each other at a distance; a substrate by which the positive electrode and …
Who is the assignee on this patent?
Tokyo Ohka Kogyo Co Ltd
What technology area does this patent fall under?
Primary CPC classification H01M10/058. Mapped technology areas include Electricity.
When was this patent published?
Publication date Tue Nov 27 2018 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 1 related publication on this page (citations in our corpus or others sharing the same primary CPC).