Polyphenylene sulfide short fiber, fibrous structure, filter felt, and bag filter
US-2020324234-A1 · Oct 15, 2020 · US
US10138577B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10138577-B2 |
| Application number | US-201515315042-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 22, 2015 |
| Priority date | May 30, 2014 |
| Publication date | Nov 27, 2018 |
| Grant date | Nov 27, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A poly(phenylene sulfide) fiber contains 1-10% by weight of a poly(phenylene sulfide) oligomer having a weight-average molecular weight of 5,000 or less, has a difference between a cold crystallization heat quantity (ΔHc) and a crystal melting heat quantity (ΔHm) during temperature rising in DSC, ΔHm−ΔHc, of 25 J/g or larger, and has an elongation of less than 40% and a strength of 3.0 cN/dtex or higher. The poly(phenylene sulfide) fiber has high heat resistance and chemical resistance and high strength and, despite this, has excellent suitability for high-order processing, e.g., thermal shapability, because the amorphous parts thereof have high molecular movability.
Opening claim text (preview).
The invention claimed is: 1. A poly(phenylene sulfide) fiber containing 1-10% by weight of a poly(phenylene sulfide) oligomer having a weight-average molecular weight of 5,000 or less, having a difference between a cold crystallization heat quantity (ΔHc) and a crystal melting heat quantity (ΔHm) during temperature rising in DSC, ΔHm−ΔHc, of 25 J/g or larger, and having an elongation of less than 40% and a strength of 3.0 cN/dtex or higher. 2. The poly(phenylene sulfide) fiber according to claim 1 , wherein the poly(phenylene sulfide) oligomer is a cyclic oligomer.
Heat treatment (heating for finishing D02J13/00) · CPC title
from polyarylene sulfides · CPC title
Selection or control of the temperature during stretching · CPC title
of other polycondensation products · CPC title
Melt spinning methods {(D01D5/0023 takes precedence)} · CPC title