Low-density clad steel sheet having excellent formability and fatigue property and manufacturing method therefor
US-2024326399-A1 · Oct 3, 2024 · US
US10119186B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10119186-B2 |
| Application number | US-201414450453-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 4, 2014 |
| Priority date | Aug 23, 2013 |
| Publication date | Nov 6, 2018 |
| Grant date | Nov 6, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a maraging steel excellent in fatigue characteristics, including, in terms of % by mass: C: ≤0.015%, Ni: from 12.0 to 20.0%, Mo: from 3.0 to 6.0%, Co: from 5.0 to 13.0%, Al: from 0.01 to 0.3%, Ti: from 0.2 to 2.0%, O: ≤0.0020%, N: ≤0.0020%, and Zr: from 0.001 to 0.02%, with the balance being Fe and unavoidable impurities.
Opening claim text (preview).
What is claimed is: 1. A maraging steel, consisting of, in terms of % by mass: C: ≤0.015%, Ni: 12.0 to 20.0%, Mo: 3.0 to 6.0%, Co: 5.0 to 13.0%, Al: 0.01 to 0.3%, Ti: 0.2 to 2.0%, O: ≤0.0020%, N: 0.0005 to 0.0020%, Zr: from 0.001 to 0.02%, and optionally one or more of: B: from 0.0010 to 0.010%, Mg: ≤0.003%, and Ca: ≤0.003% with the balance being Fe and unavoidable impurities, wherein the maraging steel comprises at least one TiN or TiCN inclusion with ZrO 2 present in a center part thereof. 2. The maraging steel according to claim 1 , the content of Zr being 0.001 to 0.008% by mass. 3. A thin steel sheet having a thickness of 0.5 mm or less and consisting of the maraging steel according to claim 1 . 4. A maraging steel consisting of, in terms of % by mass: C: ≤0.015%, Ni: 12.0 to 20.0%, Mo: 3.0 to 6.0%, Co: 5.0 to 13.0%, Al: 0.01 to 0.3%, Ti: 0.2 to 2.0%, O: ≤0.0020%, N: 0.0005 to 0.0020%, Zr: from 0.001 to 0.02%, and optionally one or more of: B: from 0.0010 to 0.010%, Mg: ≤0.003%, and Ca: ≤0.003% with the balance being Fe and unavoidable impurities, wherein the maraging steel comprises at least one TiN or TiCN inclusion with ZrO 2 present in a center part thereof and the maraging steel has a fatigue characteristic, when tested according to the method of JIS Z 2273 (2010), of 10 7 repetitions or more. 5. The maraging steel according to claim 4 , the content of Zr being 0.001 to 0.008% by mass. 6. A thin steel sheet having a thickness of 0.5 mm or less and consisting of the maraging steel according to claim 4 .
containing tungsten, tantalum, molybdenum, vanadium, or niobium · CPC title
with cobalt · CPC title
containing titanium or zirconium · CPC title
containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60 · CPC title
containing aluminium · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.