Methacrylate resin composition and molded article
US-2017313834-A1 · Nov 2, 2017 · US
US10113041B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10113041-B2 |
| Application number | US-201515326896-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 16, 2015 |
| Priority date | Jul 18, 2014 |
| Publication date | Oct 30, 2018 |
| Grant date | Oct 30, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention aims to provide a film having excellent mechanical strength and abrasion resistance. The film of the present invention contains an aromatic polyether ketone resin (I) and a fluororesin (II). The aromatic polyether ketone resin (I) has a crystallinity of 10% or higher.
Opening claim text (preview).
The invention claimed is: 1. A film comprising: an aromatic polyether ketone resin (I); and a fluororesin (II), the aromatic polyether ketone resin (I) having a crystallinity of 15% or higher. 2. The film according to claim 1 , wherein the fluororesin (II) is a copolymer of tetrafluoroethylene and a perfluoroethylenic unsaturated compound represented by the following formula (1): CF 2 ═CF—Rf 1 (1) wherein Rf 1 is —CF 3 or —ORf 2 ; and Rf 2 is a C1-C5 perfluoroalkyl group. 3. The film according to claim 1 , wherein the aromatic polyether ketone resin (I) and the fluororesin (II) have a mass ratio (I):(II) of 40:60 to 99:1. 4. The film according to claim 1 , wherein the fluororesin (II) is dispersed as particles in the aromatic polyether ketone resin (I). 5. The film according to claim 4 , wherein the fluororesin (II) has an average dispersed particle size of 3.0 μm or smaller in the aromatic polyether ketone resin (I). 6. The film according to claim 1 , wherein the aromatic polyether ketone resin (I) and the fluororesin (II) have a melt viscosity ratio (I)/(II) of 0.01 to 5.0. 7. The film according to claim 1 , wherein the fluororesin (II) has a melt flow rate of 0.1 to 100 g/10 min. 8. The film according to claim 1 , wherein the aromatic polyether ketone resin (I) is polyether ether ketone. 9. A diaphragm for speakers, comprising the film according to claim 1 . 10. A thrust washer comprising the film according to claim 1 .