System and method for removing flatness faults from a metal flat product
US-11179759-B2 · Nov 23, 2021 · US
US10086418B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10086418-B2 |
| Application number | US-201214647439-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 27, 2012 |
| Priority date | Dec 21, 2012 |
| Publication date | Oct 2, 2018 |
| Grant date | Oct 2, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
There are provided a shape-correcting and rolling method and a shape-correcting device for effectively correcting the shape of high-strength steel. The shape-correcting and rolling method includes: transferring a hot-rolled coil to a pay-off reel after cooling the hot-rolled coil or directly through a hot rolling to skin pass mill direct transfer process; unwinding the coil from the pay-off reel; correcting a shape of a strip unwound from the coil by using a heat pipe roller; and rewinding the strip as a coil.
Opening claim text (preview).
The invention claimed is: 1. A shape-correcting and rolling method for high-strength steel, comprising: performing a hot rolling to skin pass mill direct transfer process by transferring a hot-rolled coil to a pay-off reel; unwinding a strip from the coil of the pay-off reel; correcting a shape of the strip by using at least a pair of heat pipe rollers; and rewinding the strip as a coil, wherein each of the heat pipe rollers comprises a plurality of first heat pipes extending in a length direction of the heat pipe roller from an end to a center region of the heat pipe roller and a plurality of second heat pipes extending from an opposite end to the center region, the plurality of first and the plurality of second heat pipes are alternately arranged in a circumferential direction of the heat pipe roller, and the plurality of first and the plurality of second heat pipes overlap each other only in the center region in the length direction of the heat pipe roller. 2. The shape-correcting and rolling method of claim 1 , wherein prior to the correcting of the shape of the strip, the method further comprises rolling the strip at a reduction ratio of 20% to 30%. 3. The shape-correcting and rolling method of claim 2 , wherein prior to the rolling of the strip, the method further comprises removing scale from surfaces of the strip by shot blasting. 4. The shape-correcting and rolling method of claim 1 , wherein in the correcting of the shape of the strip, the strip has a temperature equal to or higher than 150° C., but lower than a phase transformation temperature. 5. The shape-correcting and rolling method of claim 4 , further comprising warm-rolling the strip. 6. The shape-correcting and rolling method of claim 1 , wherein a heat insulating process is performed on the coil during the unwinding of the coil, so as to prevent cooling of the coil. 7. The shape-correcting and rolling method of claim 1 , wherein prior to the correcting of the shape of the strip, the method further comprises heating the strip so that the strip has a uniform temperature. 8. A shape-correcting and rolling method for high-strength steel, comprising: performing a first transfer process by transferring a hot-rolled coil to a temperature adjusting unit; cooling the coil while monitoring a temperature of the coil; performing a second transfer process by transferring the coil cooled to a temperature of 150° C. or higher to a pay-off reel; unwinding a strip from the coil of the pay-off reel; correcting a shape of the strip by using a pair of heat rollers; and rewinding the strip as a coil, wherein each of the heat pipe rollers comprises a plurality of first heat pipes extending in a length direction of the heat pipe roller from an end to a center region of the heat pipe roller and a plurality of second heat pipes extending from an opposite end to the center region, the plurality of first and the plurality of second heat pipes are alternately arranged in a circumferential direction of the heat pipe roller, and the plurality of first and the plurality of second heat pipes overlap each other only in the center region in the length direction of the heat pipe roller. 9. The shape-correcting and rolling method of claim 2 , wherein the cooling of the coil comprises: measuring the temperature of the coil; and comparing the measured temperature of the coil with a predetermined temperature range so as to determine whether the measured temperature of the coil is within the predetermined temperature range. 10. The shape-correcting and rolling method of claim 9 , wherein the cooling of the coil is performed by placing the coil on a skid in a yard, and a thermocouple disposed in the skid indirectly measures the temperature of the coil by measuring a temperature of the skid heated by the coil placed on the skid. 11. A shape-correcting device for high-strength steel, the shape-correcting device comprising: a pay-off reel from which a coil is unwound; a skin pass mill correcting a strip unwound from the coil of the pay-off reel; and a coiler rewinding the strip after the strip passes through the skin pass mill, wherein the skin pass mill comprises a work roll that is a heat pipe roller in which heat pipes are installed, wherein the heat pipes comprise a plurality of first heat pipes extending in a length direction of the work roll from an end to a center region of the work roll and a plurality of second heat pipes extending from an opposite end to the center region, the plurality of first and the plurality of second heat pipes are alternately arranged in a circumferential direction of the work roll, and one of the plurality of the first heat pipes and one of the plurality of the second heat pipes overlap each other only in the center region in the length direction of the work roll. 12. The shape-correcting device of claim 11 , wherein the heat pipes are uniformly arranged in the circumferential direction of the work roll at a predetermined insertion depth. 13. The shape-correcting device of claim 11 , wherein a heating device is disposed between the pay-off reel and the skin pass mill so as to heat the strip to a temperature equal to or higher than 150° C. but lower than a phase transformation temperature. 14. The shape-correcting device of claim 11 , further comprising a shot blaster configured to shoot steel balls having a micrometer (μm) size toward the strip and a rolling mill disposed behind the shot blaster to roll the strip, wherein the shot blaster and the rolling mill are disposed between the pay-off reel and the skin pass mill. 15. The shape-correcting device of claim 11 , further comprising at least one additional pay-off reel and a heat insulation cover, wherein when one of the pay-off reels is operated, the heat insulation cover covers the remaining pay-off reel that is not operated and a coil disposed on the remaining pay-off reel.
Hot rolling · CPC title
heating internally · CPC title
by rollers (B21D1/06 takes precedence) · CPC title
Flattening; Dressing; Flexing · CPC title
Winding-up or coiling · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.