Hot melt adhesives and uses thereof
US-2024228837-A1 · Jul 11, 2024 · US
US10066129B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10066129-B2 |
| Application number | US-201314425187-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 30, 2013 |
| Priority date | Sep 4, 2012 |
| Publication date | Sep 4, 2018 |
| Grant date | Sep 4, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention provides an anti-fouling pressure-sensitive adhesive sheet and anti-fouling treatment method capable of preventing peeling from overlapping portions when adjacent anti-fouling pressure-sensitive adhesive sheets are attached by allowing end portions thereof to overlap each other. The anti-fouling pressure-sensitive adhesive sheet of the present invention includes a base material layer; a pressure-sensitive adhesive layer provided on one side of the base material layer; and an anti-fouling layer provided on another side of the base material layer, wherein the anti-fouling pressure-sensitive adhesive sheet has, at an end portion thereof, a bonding margin including parts of the base material layer and the pressure-sensitive adhesive layer, the parts extending beyond the anti-fouling layer.
Opening claim text (preview).
The invention claimed is: 1. An anti-fouling treatment method for a structure, comprising sequentially attaching three or more anti-fouling pressure-sensitive adhesive sheets onto a surface of a structure to be subjected to anti-fouling treatment so that a bonding margin of a preceding anti-fouling pressure-sensitive adhesive sheet is overlapped by a pressure-sensitive adhesive layer surface of a succeeding anti-fouling pressure-sensitive adhesive sheet, wherein each anti-fouling pressure-sensitive adhesive sheet comprises a base material layer; a pressure-sensitive adhesive layer provided on one side of the base material layer; and an anti-fouling layer provided on another side of the base material layer, wherein the anti-fouling pressure-sensitive adhesive sheet has, at only one end portion thereof, the bonding margin including parts of the base material layer and the pressure-sensitive adhesive layer, the parts extending beyond the anti-fouling layer, and wherein an adhesive strength between the base material layer-side surface of the bonding margin and the pressure-sensitive adhesive layer is higher than an adhesive strength between the surface of the structure to be subjected to anti-fouling treatment and the pressure-sensitive adhesive layer. 2. The anti-fouling treatment method for a structure according to claim 1 , wherein the bonding margin is overlapped by the pressure-sensitive adhesive layer surface so that an overlapping width of the anti-fouling pressure-sensitive adhesive sheets is larger than a width of the bonding margin, and wherein the anti-fouling treatment method further comprises cutting off an overlapping portion beyond the bonding margin. 3. The anti-fouling treatment method for a structure according to claim 1 , wherein the bonding margin has a base material layer-side surface thereof subjected to easy-adhesion treatment. 4. The anti-fouling treatment method for a structure according to claim 1 , wherein the bonding margin has, at an end portion thereof, an inclined surface that is inclined so as to have a thickness decreasing from a base material layer-side surface toward a pressure-sensitive adhesive layer-side surface. 5. The anti-fouling treatment method for a structure according to claim 1 , wherein the anti-fouling layer is a silicone-based resin layer or fluorine-based resin layer each containing a silicon oil and/or liquid paraffin. 6. The anti-fouling treatment method for a structure according to claim 1 , wherein a 180° peeling adhesive strength of the pressure-sensitive adhesive layer at 23° C. and a tension speed of 300 mm/min is 15 N/20 mm or less, and a 180° peeling adhesive strength between the base material layer-side surface of the bonding margin and the pressure-sensitive adhesive layer at 23° C. and a tension speed of 300 mm/min is 20N/20 mm or more.
Presence of (meth)acrylic polymer · CPC title
Hull protection specially adapted for vessels; Cleaning devices specially adapted for vessels {(inhibiting corrosion of metals by anodic or cathodic protection C23F13/00)} · CPC title
Methods of surface bonding and/or assembly therefor · CPC title
in the substrate · CPC title
Adhesive articles, e.g. adhesive tapes · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.