Process and apparatus for making a mineral melt

US10040712B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-10040712-B2
Application numberUS-93437809-A
CountryUS
Kind codeB2
Filing dateMar 26, 2009
Priority dateMar 27, 2008
Publication dateAug 7, 2018
Grant dateAug 7, 2018

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

The present invention relates to an apparatus and a method of making a mineral melt, the method comprising the steps of providing a circulating combustion chamber (1); injecting fuel, preheated mineral material and combustion gas into the circulating combustion chamber (1); combusting the fuel in the circulating combustion chamber (1) thereby melting the mineral material to form a mineral melt and generating exhaust gases; separating the exhaust gases from the mineral melt, collecting the mineral melt (9) and passing the exhaust gases (10) to a heat exchange system, the method being characterised in that the mineral material comprises a first mineral material and a second mineral material wherein the first mineral material has a higher sintering temperature than the second mineral material and the first and second mineral materials are provided separately to the heat exchange system, wherein the first mineral material is preheated through contact with the exhaust gases and subsequently the second mineral material is preheated through contact with the exhaust gases and the preheated first mineral material.

First claim

Opening claim text (preview).

The invention claimed is: 1. A method of making a mineral melt, the method comprising the steps of: providing a circulating combustion chamber and a heat exchange system; heating mineral material comprising first and second mineral materials; injecting fuel, the heated mineral material, and combustion gas into the circulating combustion chamber; combusting the fuel in the circulating combustion chamber, thereby melting the heated mineral material to form a mineral melt and generate exhaust gases; separating the exhaust gases from the mineral melt, collecting the mineral melt, and passing the exhaust gases to the heat exchange system; wherein prior to being injected into the circulating combustion chamber, the first and second mineral materials are provided separately to the heat exchange system, and wherein said first mineral material is a raw mineral material and said second mineral material is bonded mineral wool; and wherein the first mineral material has a higher sintering temperature than the second mineral material; and wherein the first mineral material is heated through contact with the exhaust gases before the second mineral material is heated through contact with the exhaust gases and the heated first mineral material. 2. A method according to claim 1 , additionally comprising a step of: flowing the collected mineral melt through an outlet in the circulating combustion chamber to a centrifugal fiberising apparatus to form mineral fibres. 3. A method according to claim 2 , wherein the mineral fibres are selected from the group consisting of rock, stone and slag fibres and have a composition, by weight of oxides, comprising below 10% NaO+K 2 O, above 20% CaO+MgO, above 3% iron oxide, and below 50% SiO 2 . 4. A method according to claim 1 , wherein the heated mineral material comprises between 5 and 70% by weight, preferably between 10 and 60% by weight and most preferably between 25 and 50% by weight of the second mineral material. 5. A method according to claim 1 , wherein the heat exchange system comprises a first cyclone preheater and a first conduit from the circulating combustion chamber to the first cyclone preheater through which the exhaust gases pass, wherein the method comprises injecting the first and second mineral materials into a first conduit; wherein said injection of the first mineral material into the first conduit is at a position closer to the circulating combustion chamber than said injection of the second mineral material into the first conduit. 6. A method according to claim 5 , comprising: injecting the first mineral material into a second conduit so that the first mineral material undergoes initial heating in a second cyclone preheater prior to being injected into the first conduit. 7. A method according to claim 6 , wherein the first mineral material is initially heated in the second cyclone preheater to a temperature in the range of 400-500° C. 8. A method according to claim 1 , wherein the exhaust gases are at a temperature in the range of 1300 to 1500° C. at the contact with the first mineral material. 9. A method according to claim 1 , wherein, during heating, the second mineral material is heated to a temperature of at least 800° C., preferably 850 to 950° C. through contact with the exhaust gases and the heated first mineral material. 10. The method of claim 1 , wherein the bonded wool material is selected from the group consisting of bonded rock fibres, bonded stone fibres, and bonded slag fibres. 11. A method of making a mineral melt, the method comprising the steps of: providing a circulating combustion chamber and a heat exchange system; heating mineral material comprising first and second mineral materials; injecting fuel, the heated mineral material, and combustion gas into the circulating combustion chamber; combusting the fuel in the circulating combustion chamber, thereby melting the heated mineral material to form a mineral melt and generate exhaust gases; separating the exhaust gases from the mineral melt, collecting the mineral melt, and passing the exhaust gases to the heat exchange system, wherein the heat exchange system comprises a first cyclone preheater and a first conduit from the circulating combustion chamber to the first cyclone preheater through which the exhaust gases pass; wherein prior to being injected into the circulating combustion chamber, the first and second mineral materials are provided separately to the heat exchange system, and wherein said first mineral material is a raw mineral material and said second mineral material is bonded mineral wool; and wherein the first mineral material has a higher sintering temperature than the second mineral material; and heating the first mineral material through contact with the exhaust gases; and subsequently heating the second mineral material through contact with the exhaust gases and the heated first mineral material; wherein the method comprises injecting the first and second mineral materials into a first conduit; wherein said injection of the first mineral material into the first conduit is at a position closer to the circulating combustion chamber than said injection of the second mineral material into the first conduit.

Assignees

Inventors

Classifications

  • Preheating · CPC title

  • for pulverulent fuel · CPC title

  • by charging the ingredients into a flame, through a burner or equivalent heating means used to heat the melting furnace · CPC title

  • C03B5/12Primary

    in shaft furnaces {(C03B5/02 takes precedence)} · CPC title

  • Cross-Sectional Technologies · mapped topic

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US10040712B2 cover?
The present invention relates to an apparatus and a method of making a mineral melt, the method comprising the steps of providing a circulating combustion chamber (1); injecting fuel, preheated mineral material and combustion gas into the circulating combustion chamber (1); combusting the fuel in the circulating combustion chamber (1) thereby melting the mineral material to form a mineral melt …
Who is the assignee on this patent?
Hansen Peter Farkas Binderup, Hansen Lars Elmekilde, Bollund Lars, and 2 more
What technology area does this patent fall under?
Primary CPC classification C03B5/12. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue Aug 07 2018 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).